Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 252 - 274 °C | 485 - 525 °F | |
PTS PCA-3013 High Flow PC/PBT Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 263 - 274 °C | 505 - 525 °F | |
Teknor Apex Chemlon® 182 Nylon 66, Non-Halogenated Notes: General Purpose; U.L. 94 V-O at 0.57 mm; Colorable; Flame Retardant Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 340G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Front Barrel Temperature | 246 - 274 °C | 475 - 525 °F | |
CTC X-PRO PP 100 P1015 Polypropylene Homopolymer X-PRO PP 1015 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Front Barrel Temperature | 227 - 274 °C | 440 - 525 °F | |
LTL Color Compounds ColorFast® FRPA100X Polycarbonate-ABS Alloy V-0 rated polycarbonate-ABS alloy, excellent toughness and light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Front Barrel Temperature | 227 - 274 °C | 440 - 525 °F | |
LTL Color Compounds ColorFast® JCT1000 Polycarbonate-ABS-SMA Alloy Unique PC/ABS/SMA alloy with improved processing and reduced plate-outAll information provided by LTL Color Compounders, Inc. |