| Category | Polymer , Thermoplastic , Nylon , Nylon 610 , Nylon 610, Glass Reinforced |
| Manufacturer | Teknor Apex Company |
| Trade Name | Chemlon® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.45 g/cc | 1.45 g/cc | ASTM D792 |
| Water Absorption | 0.17 % | 0.17 % | 24 hr; ASTM D750 |
| Linear Mold Shrinkage | 0.0010 - 0.0030 cm/cm | 0.0010 - 0.0030 in/in | ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 183 MPa | 26500 psi | ASTM D638 |
| Elongation at Break | 2.5 % | 2.5 % | ASTM D638 |
| Elongation at Yield | 2.5 % | 2.5 % | ASTM D638 |
| Flexural Strength | 259 MPa | 37500 psi | ASTM D790 |
| Flexural Modulus | 9.65 GPa | 1400 ksi | ASTM D790 |
| Izod Impact, Notched | 1.87 J/cm <br>@Temperature 22.8 °C |
3.50 ft-lb/in <br>@Temperature 73.0 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 216 °C | 420 °F | Unannealed; ASTM D648 |
| Flammability, UL94 | HB <br>@Thickness 0.810 mm |
HB <br>@Thickness 0.0319 in |
|
| Oxygen Index | 25 % | 25 % | ASTM D2863 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 235 - 252 °C | 455 - 485 °F | |
| Middle Barrel Temperature | 246 - 268 °C | 475 - 515 °F | |
| Front Barrel Temperature | 257 - 274 °C | 495 - 525 °F | |
| Nozzle Temperature | 252 - 279 °C | 485 - 535 °F | |
| Melt Temperature | 223 °C | 433 °F | |
| 252 - 277 °C | 485 - 530 °F | Processing Temperature | |
| Drying Temperature | 79.4 °C | 175 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Suggested Moisture, max | 0.2 | |
| Suggested Regrind, max | 25 |