Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Start Point: 250°C |
Kingfa MAC-601 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Front Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Start Point: 255°C |
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Injection Molding |
LG Chemical LUMID GP1200A(W) PA6, Medium Viscosity Feature: Injection Molding, PA6, Medium ViscosityApplication: Industrial Material, Sport PartsCAS No. 25038-54-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Injection Molding |
LG Chemical LUMID HI5001AH PA6/PO, High Melt Strength, High Barrier property, CaCl2 Resistance Feature: Injection Molding, PA6/PO, High Melt Strength, High Barrier property, CaCl2 ResistanceApplication: Automotive (Fuel System Tube)CAS No. 25038-54-4, 9010-79-1 and 9002-88-4Information provid.. |
|||
Front Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Injection Molding |
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG .. |
|||
Front Barrel Temperature | 240 - 265 °C | 464 - 509 °F | Injection Molding |
LG Chemical LUMID LW4203A(W) PA6+GF/MF20%, Low Warpage Feature: Injection Molding, PA6+GF/MF20%, Low WarpageApplication: Automotive Parts (Engine Cover)CAS No. 25038-54-4, 13983-17-0 and 65997-17-3Information provided by LG Chemical |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical Lupox® PBT-GP-2306FA 30% GFR Flame Retardant, UV Stabilized PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 240 - 280 °C | 464 - 536 °F | Injection Molding |
Styrolution Luran® S 777 K ASA Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | Zone 3 |
Eurostar Staramide BG5H PA6, 25% Glass Filled, Injection Molded BG5H is a Heat Stabilized, 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Front Barrel Temperature | 240 - 260 °C | 464 - 500 °F | Zone 3 |
Eurostar Starflam P10002E PA6, Injection Molded Starflam P10002E is a Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding Resin (also known as P1000Z220 or PA6 U2 Z22)Information provided by Polymer Tec.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® M344 BLK Nylon 66, Flame Retardant, DAM Vydyne® M344 BLK is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has Underwr.. |
|||
Front Barrel Temperature | 240 - 270 °C | 464 - 518 °F | |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |