Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Front Barrel Temperature = 374 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Front Barrel Temperature 190 °C
374 °F
Multibase TPSiV™ 3340-65A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical ALPHALAC SG970 HIPS
Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical GPPS 20HR(E) PS, High Transparency, Heat Resistance
Description: Injection Molding, PS, High Transparency, Heat ResistanceApplication: PSP, Food Tray, Electric/Electrical Component, CoatingCAS: 9003-53-6Information provided by LG Chemical
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical HIPS MI730 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Front Barrel Temperature 190 - 200 °C
374 - 392 °F
LG Chemical LUCEL HI-515 High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Front Barrel Temperature 190 - 200 °C
374 - 392 °F
LG Chemical LUCEL HI-525 High Impact POM, Unreinforced
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Front Barrel Temperature 190 - 200 °C
374 - 392 °F
Injection Molding
LG Chemical LUCEL N109LD POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Copier, Watch, Clock, VCR, Printer Parts, etc.CAS No. 66455-31-0Information provided by LG Chemical
Front Barrel Temperature 190 - 200 °C
374 - 392 °F
Injection Molding
LG Chemical LUCEL N109WR POM, Chemical Resistance
Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical
Front Barrel Temperature 190 - 215 °C
374 - 419 °F
LG Chemical Lucet® N109 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Front Barrel Temperature 190 - 250 °C
374 - 482 °F
Injection
Inno-Comp INNOPOL® CS 2-3110 TO BU 10% Talc Filled Polypropylene Copolymer
INNOPOL® CS 2-3110 TO BU is a 10% talc-filled, black colored and UV stabilized compound based on polypropylene block-copolymer.INNOPOL® CS 2-3110 TO BU is developed for producing injection mol..
Front Barrel Temperature 190 °C
374 °F
Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin
HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and c..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical 82TR SAN, High Transparency, Heat Resistance, Chemical Resistance
Feature: Injection Molding, SAN, High Transparency, Heat Resistance, Chemical ResistanceApplication: Refrigerator Sleeves, MiscellaneousCAS No. 9003-54-7Information provided by LG Chemical
Front Barrel Temperature 190 °C
374 °F
Metering zone
Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Front Barrel Temperature 190 - 220 °C
374 - 428 °F
Extrusion
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r..
Front Barrel Temperature 190 - 230 °C
374 - 446 °F
Borealis Beta (ß)-PP™ BE60-7032 Grey Polypropylene Homopolymer for Pressure Pipes, Fittings and Sheets
Beta(ß)-PP BE60-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer with fine grained ß-modification crystalline structure leading to excellent impact strength even at lo..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Borealis Borstar® HE3494-LS Dark Blue High Density Polyethylene for Drinking Water Pipes
Borstar HE3494-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Tisan TISOPLEN® Flame Retardant (V0). Heat Stabilized, Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Borealis Borstar® HE3492-LS Yellow-Orange High Density Polyethylene for Natural Gas Pipes
Borstar HE3492-LS is a yellow-orange, cadmium free, high density polyethylene compound classified as a MRS 10.0 material (PE100) produced with the advanced Borstar technology. It includes a combina..
Front Barrel Temperature 190 - 220 °C
374 - 428 °F
Unitika TERRAMAC HV-6250H Polylactic Acid (PLA)
Foam, Extrusion, blow, and foam sheet grades. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Tisan TISOPLEN® 20% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA)
Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Unitika TERRAMAC TE-8300 Polylactic Acid (PLA)
High-durability, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Tisan TISOPLEN® 30% Calcite Filled Heat Stabilized Homopolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Front Barrel Temperature 190 °C
374 °F
Injection
Alliance Polymers Viprene™ G80A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G80A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Front Barrel Temperature 190 °C
374 °F
Injection
Alliance Polymers Viprene™ G85A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G85A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Pre-3. Region Temperature
Tisan TISOPLEN® 25% Glass Fiber Reinforced Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene
TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical HIPS MI750 PS, Impact Modified
Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica..
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
LG Chemical XG570 MABS, Anti-Scratch, High Impact, High Flow
Feature: Injection Molding, Anti-Scratch, High Impact, High FlowApplication: LCD TV Stand Base, Audio/Video HousingCAS No. 9010-94-0Information provided by LG Chemical