Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer
(discontinued **) Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt .. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Honeywell Aegis™ PL220HS High Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL220HS is a high viscosity, heat stabilized, flexible nylon 6 especially suited to the production of large diameter extrusion or blow molding profiles offering a combination of g.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT 3055D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical KEYFLEX BT HB9242D Ester Type TPE Description: TPC-ET, Blow Moldable, Low Modulus, Black ColorApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5 and 1333-86-4Information provided by LG Chemical |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX GP-5106F General Purpose PBT, 10% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Injection Molding |
LG Chemical LUMAX GP5106FI PBT+ABS+GF10%, Flame Retardant Description: Injection Molding Grade, PBT+ABS+GF10%, Flame Retardant, Impact Modified, Dimensional StabilityApplication: E&E (Switch)CAS: 9003-56-9, 68928-70-1, 65997-17-3, 24968-12-5, 9003-54-7 an.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX GP-5200 General Purpose PBT, 20 % Polymer Alloy LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX HF-5306F High Flow PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical LUMAX HR-5306F Heat Resistant PBT, 30% Polymer Alloy, Weather Resistant, Flame Retardant LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
LG Chemical LUPOS HR-2307 Heat Resistant SAN, 30% Glass Fiber Reinforced LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
LG Chemical Lupox® PBT-LW5303 30% Glass Filled Low Warp PBT Low Warpage. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical LUPOY EF5001RFT PC/ABS Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, EU Eco-Label compliantApplication: Display housingCAS: 103598-77-2, 9003-56-9 and 125997-21-9Information provided by LG Chemical.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR409E ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR409H ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior Housing (Switch Panel Housing etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provided by LG Ch.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Injection Molding |
LG Chemical XR419 ABS, Heat Resistance, Chemical Resistance Feature: Injection Molding, Heat Resistance, Chemical ResistanceApplication: Automotives Interior Housing (Ventgrille Etc)CAS No. 25120-20-1, 9003-56-9, 25747-74-7, and 31621-07-5Information provide.. |
|||
Front Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | Start Point: 240°C |
Kingfa MAC-501DY Modified PC/ABS Alloy Features:Excellent balance propertiesGood low temperature impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile license platePower toolComp.. |
|||
Front Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
LG Chemical LUPOY GN-5001TF Halogen Free PC/ABS Alloy, High Flow, Flame Retardant Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
Solvay TECHNYL® C 218 V33 PA6, 33% glass fiber, Eh 0 Description: Polyamide PA6, reinforced with 33% of glass fiber, heat stabilized, for injection molding.Applications: It has good mechanical properties, it is used in all sectors of industry, offerin.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | |
Solvay Technyl® C218V30 30% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 230 - 250 °C | 446 - 482 °F | |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Front Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Pre-3. Region Temperature |
Tisan TISESTER® 15% Glass Fiber Reinforced Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Front Barrel Temperature | 240 - 250 °C | 464 - 482 °F | Zone 3 |
Eurostar Staramide BST03 PA6, Impact Modified, Injection Molded BST03 is an Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Front Barrel Temperature | 245 - 250 °C | 473 - 482 °F | |
Solvay TECHNYL® 1015CR PA6, DRY Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |
|||
Front Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |