Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1001-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Facias, claddings, and rocker panelsBodyside moldingsStep pads and bumper componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1004-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1004-625UV Thermoplastic Polyolefin, UV Stabilized, Interior DX9 Black Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2400-647UV Thermoplastic Polyolefin, UV Stabilized, 8798NM Grey Applications: Bumper rub stripsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT3080-81 Thermoplastic Polyolefin, UV Stabilized, ACRA Titanium Applications: Step padsHitch padsScuff padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products FT4600-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Scuff platesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P100-01 Polypropylene Homopolymer, Black Applications: Wire harnessesTrim componentsUnderhood applicationsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products P257-01 Polypropylene Copolymer, Black Applications: Splash shield and fender linersElectrical enclosuresUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 204 - 227 °C | 399 - 441 °F | |
PolyOne Versaflex™ FFC 2882-50 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-50 is designed to pass several fatty food extraction conditions identified in EU Directive 82/711/EEC. Versaflex™ FFC 2882-50 will also overmold and co-extrude to polypropylene.. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G10 ABS, 10% Glass Reinforced Acrylonitrile Butadiene Styrene, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G5 ABS, 5% Glass Reinforced Acrylonitrile Butadiene Styrene, 5% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7690-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7690-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G15 ABS, 15% Glass Reinforced Acrylonitrile Butadiene Styrene, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Front Barrel Temperature | 210 - 227 °C | 410 - 440 °F | |
Polymer Resources ABS-G20 ABS, 20% Glass Reinforced Acrylonitrile Butadiene Styrene, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G2711-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2711-1000-00 is an easy process compound designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - O.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7970-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Front Barrel Temperature | 188 - 227 °C | 370 - 441 °F | |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-69/10/E High performance polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Fiberfil® J-69/30/E/M High performance polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Front Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Front Barrel Temperature | 221 - 227 °C | 430 - 440 °F | |
Teknor Apex Telcar® TL-8431 Thermoplastic Elastomer Notes: RoHS Compliant Uses: Appliance Wire Insulation; Appliance Wire Jacketing; Cable Jacketing; Connectors; Flexible Cord Jacketing; Electrical/Electronic Applications; Industrial Cable Jacketing;.. |
|||
Front Barrel Temperature | 199 - 227 °C | 390 - 440 °F | |
RheTech Products HP501-00 High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |