Processing Properties | Metric | English | Comments |
---|---|---|---|
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/10/CC/30/E NATL Polypropylene Homopolymer, 10% FiberGlass and 30% Calcium Carbonate Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/10/E/M Polypropylene Homopolymer, 10% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/15/E Polypropylene Homopolymer, 15% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/20/E/NS Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, NSF listed Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/30/E/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/30/FR Polypropylene Homopolymer, 30% Glass Fiber Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-60/40/E Polypropylene Homopolymer, 40% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® M-2450 Polypropylene Copolymer Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/TC/13 BL8860 Polypropylene Homopolymer, 13% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/TC/24/D/HS Polypropylene Homopolymer, Talc Filled, Heat Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-60/TC/40/OP WT2595 Polypropylene Homopolymer, 40% Talc Filled, high opacity Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Kraton® D2109 DS-N (SBS) Compound Description: Kraton D2109 DS-N is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Front Barrel Temperature | 188 - 199 °C | 370 - 390 °F | |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-61/30/FR Polypropylene Copolymer, 30% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-62/30/E8 Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-68/25/E/SD Polypropylene Copolymer, 25% Glass Fiber Reinforced, Chemically coupled, with static dissipation Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Teknor Apex Flexalloy® 9300-70 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, Oil Resistant, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather R.. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Elastocon TPE Technologies Elastocon® 8078NL Thermoplastic Elastomer Elastocon® 8078NL is a colorable thermoplastic elastomer formulated for applications that require rubber-like properties and a scratch and mar resistant surface finish. Elastocon® 8078NL is FDA c.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-35 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8271-55 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-35MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 185 - 199 °C | 365 - 390 °F | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-68/20/E Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |