Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.04 g/cc | 1.04 g/cc | ASTM D792 |
Water Absorption | 0.030 % | 0.030 % | 24 hr; ASTM D570 |
Linear Mold Shrinkage | 0.0030 cm/cm @Thickness 3.17 mm |
0.0030 in/in @Thickness 0.125 in |
ASTM D955 |
0.0040 cm/cm @Thickness 6.35 mm |
0.0040 in/in @Thickness 0.250 in |
ASTM D955 | |
Melt Flow | 6.0 g/10 min | 6.0 g/10 min | 230/2.16 (typical); ASTM D1238 |
Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, Rockwell R | 100 - 110 | 100 - 110 | ASTM D785 |
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Elongation at Yield | 3.5 % | 3.5 % | ASTM D638 |
Tensile Modulus | 4.14 GPa | 600 ksi | ASTM D638 |
Flexural Strength | 93.1 MPa | 13500 psi | ASTM D790 |
Flexural Modulus | 3.72 GPa | 540 ksi | Secant; ASTM D790 |
Izod Impact, Notched | 0.641 J/cm @Thickness 3.17 mm |
1.20 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 157 °C | 315 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 152 °C | 305 °F | ASTM D648 |
Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Middle Barrel Temperature | 204 - 227 °C | 400 - 440 °F | |
Front Barrel Temperature | 182 - 199 °C | 360 - 390 °F | |
Nozzle Temperature | 182 - 193 °C | 360 - 380 °F | |
Melt Temperature | 199 - 232 °C | 390 - 450 °F | |
Mold Temperature | 32.2 - 71.1 °C | 90.0 - 160 °F | |
Drying Temperature | 76.7 °C | 170 °F | Drying not normally required |
Dry Time | 2 hour | 2 hour | Drying not normally required |
Moisture Content | <= 0.20 % | <= 0.20 % | recommended for molding |
Back Pressure | 0.000 - 0.689 MPa | 0.000 - 100 psi |