Polymer Property : Middle Barrel Temperature = 285 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY HI1002ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY SC1004A PC
Description: Injection Molding, PC, General Purpose, High Toughness, Chemical resistance, High Impact (at Low Temperature)Application: Mobile Phone HousingCAS: 103598-77-2 and 143106-82-5Information..
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY SC1004L PC, High Impact
Description: Injection Molding, PC, General Purpose, High Flow, High Impact, Chemical ResistanceApplication: Mobile Phone HousingInformation provided by LG Chemical
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
Description: Injection Molding, PC+GF20%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY SC2302 PC+GF30%, High Impact
Description: Injection Molding, PC+GF30%, Good Toughness, Good Impact, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 65997-17-3Information provided by LG Chemical
Middle Barrel Temperature 285 - 300 °C
545 - 572 °F
Injection Molding
LG Chemical LUPOY SC3154 PC+GF15%
Description: Injection Molding, PC+GF15%, General Purpose, Good Toughness, Dimensional Stability, Good Surface, Chemical ResistanceApplication: Mobile Phone Housing and ComponentsInformation provide..
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY GN1004FA PC, Halogen Free, Flame Retardant, Chemical Resistance
Description: Injection Molding, PC, Halogen Free Flame Retardant, Chemical Resistance, High Impact at Low TemperatureApplication: IT/OA Housing and ComponentsCAS: 103598-77-2 and 143106-82-5Informat..
Middle Barrel Temperature 285 - 302 °C
545 - 576 °F
A. Schulman ComAlloy Comtuf® 602 Nylon 6/6, High Impact Modified
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Middle Barrel Temperature 285 - 302 °C
545 - 576 °F
A. Schulman ComAlloy Comtuf® 604 Nylon 6/6, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Middle Barrel Temperature 285 - 302 °C
545 - 576 °F
A. Schulman ComAlloy Comtuf® 607 Nylon 6/6, Impact Modified, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
Middle Barrel Temperature 285 - 305 °C
545 - 581 °F
Injection Molding
LG Chemical LUPOY SC1004ML PC, High Impact
Description: Injection Molding, PC, General Purpose, High Impact, Good Coloring, Chemical ResistanceApplication: Mobile Phone HousingCAS: 103598-77-2 and 9046-16-6Information provided by LG Chemical..
Copyright © lookpolymers.com All Rights Reserved