Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 285 - 302 °C | 545 - 576 °F | |
A. Schulman ComAlloy Comtuf® 602 Nylon 6/6, High Impact Modified Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Middle Barrel Temperature | 285 - 302 °C | 545 - 576 °F | |
A. Schulman ComAlloy Comtuf® 604 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Middle Barrel Temperature | 285 - 302 °C | 545 - 576 °F | |
A. Schulman ComAlloy Comtuf® 607 Nylon 6/6, Impact Modified, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Middle Barrel Temperature | 291 - 302 °C | 556 - 576 °F | |
A. Schulman ComAlloy Hiloy® 628 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 291 - 302 °C | 556 - 576 °F | |
A. Schulman ComAlloy Hiloy® 629 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 291 - 302 °C | 556 - 576 °F | |
A. Schulman ComAlloy Hiloy® 627 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |