Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 224 - 235 °C | 435 - 455 °F | |
PTS PCA-1010HF High Flow Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 224 - 235 °C | 435 - 455 °F | |
PTS PCA-1011 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 224 - 235 °C | 435 - 455 °F | |
PTS PCA-1012 High Impact Polycarbonate/ABS Alloy Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Injection Molding |
LG Chemical LUMAX GN5006FC PBT+ABS, Heat Resistance Description: Injection Molding, PBT+ABS, Halogen Free Flame RetardantApplication: E&E (Connector)CAS: 9003-56-9, 9003-54-7 and 24968-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
Solvay Technyl® C 206 Nylon 6, EH0 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
Solvay Technyl® C 206 Nylon 6, EH50 Unreinforced Plyamide PA6, standard for fast cycling, for injection molding.Technyl C 206 has high fluidity and good mold release, favored by a high crystallization rate. It is specially suitable f.. |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Compression Zone |
Solvay Technyl® C206F Unfilled, Fast Cycle Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
Solvay Technyl Starâ„¢ S 218 V30 30% Glass Reinforced Nylon 6 Heat stabilized, low viscosity, injection grade.Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | |
Solvay Technyl Starâ„¢ S 60G1 V30 30% Glass Reinforced Nylon 6, Flame Retardant This Halogen free flame retardant grade, based on high fluidity Technyl Star, combines excellent all-round mechanical properties with outstanding flame retardancy and electrical performance. This pr.. |
|||
Middle Barrel Temperature | 225 - 235 °C | 437 - 455 °F | Mid-2. Region Temperature |
Tisan TISBLEND® PC/ABS TISBLEND has a wide area of application in electric/electronic, food packaging, information technology, information technology, medical and automotive industries. General Specification include: High.. |