Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 4; Cylinder |
Premix Thermoplastics PRE-ELEC® PE 1292 PRE-ELEC PE 1292 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 5; Cylinder |
Premix Thermoplastics PRE-ELEC® PET 1451 PRE-ELEC PET 1451 is a conductive thermoplastic compound based on PETG. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PET 14.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 3; Cylinder |
Premix Thermoplastics PRE-ELEC® PS 1324 PRE-ELEC PS 1324 is a conductive thermoplastic compound based on polystyrene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC .. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
Gichem GILAC G160 Acrylonitrile Butadiene Styrene
(discontinued **) ABS very high fluidity, good resilience. Medium-High Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Gichem GIBLEND E45400 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Middle Barrel Temperature | 220 °C | 428 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E623 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E689 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | |
Gromax 1155LL TPE 1155LL is medium modulus grade with nominal Durometer hardness of 55D. It contains color stable antioxidants. It can be processed by thermoplastic processing techniques like injection molding and ex.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Start Point: 240°C |
Kingfa MAC-451 UV Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Middle Barrel Temperature | 220 - 275 °C | 428 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5001RFD PC/ABS, High Impact Description: Injection Molding, PC/ABS, General Purpose, High Impact, Halogen Free Flame retardantApplication: IT&OA (Notebook PC housingCAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provid.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samsung Cheil Industries Starex® SR-0300 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samsung Cheil Industries Starex® SR-0320 High Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samsung Cheil Industries Starex® SV-0167EX Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | |
Samyang Tribit® 1503 Polybutylene Terephthalate Characteristics:High flow & processabilityApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provid.. |
|||
Middle Barrel Temperature | 220 - 270 °C | 428 - 518 °F | mass temperature |
Borealis BJ100HP Polypropylene Copolymer BJ100HP is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wi.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 1913 AC Ethylene and 13% Methyl Acrylate Copolymer Elvaloy® 1913 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | Extrusion lamination |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Mid-2. Region Temperature |
Tisan TISESTER® 15% Glass Fiber Reinforced and Heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Middle Barrel Temperature | 220 - 250 °C | 428 - 482 °F | Mid-2. Region Temperature |
Tisan TISESTER® 30% Glass Fiber Reinforced and heat Stabilized Polybutylene Terephthalate TISESTER has a wide area of application in automotive, electric/electronics and durable goods industries. General Specifications include: Excellent surface appearanceHigh corrosion and abrasion resi.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 6 15% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Mid-2. Region Temperature |
Tisan TISLAMID® 6 Flame Retardant (V0) Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
Lubrizol Isoplast® 101 Engineering Thermoplastic Polyurethane Resin ISOPLAST® 101 is an engineering thermoplastic polyurethane resin.Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product li.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | |
DuPont Bynel® 30E670 Adhesive Resin Bynel® Series 3000 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p.. |
|||
Middle Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Pipe Extrusion |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Middle Barrel Temperature | 220 °C | 428 °F | For coextrusion with EVA or EVOH. |
DuPont Bynel® 41E712 Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |