Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRP102-01 Polypropylene, Flame Retardant, Black Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Polymer Resources ABS-FR-[color]-UV Flame Retardant ABS, UV-stabilized Flame Retardant Acrylonitrile Butadiene Styrene, UV-stabilizedFeatures: • Flame Retardant • Self Extinguishing • Good UV ResistanceProcess: Injection MoldingNotes: All physical, mechanical and.. |
|||
Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
PTS Trilac® FR3800 Flame Retardant ABS Resin, RoHS Compliant Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 193 - 210 °C | 380 - 410 °F | |
Fiberfil® PP-61/VO/NH Polypropylene Copolymer, Flame Retardant, non-halogenated, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HI100X ABS, High Impact, Semi-Transparency, Flexible Feature: Injection Molding, High Impact, Semi-Transparency, FlexibleApplication: Artificial Nails, Miscellaneous Goods)CAS No. 9010-94-0Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HI110 ABS, High Impact, Chemical Resistance Feature: Injection Molding, High Impact, Chemical ResistanceApplication: Edge of Furniture ApplicationsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical KEYFLEX BT 1140D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
LG Chemical LUCEL CF-620 Electrically Conductive POM, 20% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Middle Barrel Temperature | 188 - 210 °C | 370 - 410 °F | |
Kostat 7440 Conductive ABS Compound KOSTAT 7440 is a conductive thermoplastic compound based on Acrylonitrile Butadiene Styrene and a special carbon black. KOSTAT 7440 is not dependant on atmospheric conditions and is used for ESD in.. |
|||
Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
LTL Color Compounds ColorFast® FRA203 ABS Business machinery V0 ABS with excellent indoor light stabilityAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 200 - 210 °C | 392 - 410 °F | |
Lavergne VYTEEN ABS 2904 Acrylonitrile Butadiene Styrene Vyteen ABS 2904 is a black recycled ABS high impact flow terpolymer with balanced impact/stiffness properties designed for injection molding applications.Features: -Excellent resilience -Good proc.. |
|||
Middle Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4165 Thermoplastic Elastomer A highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4165 is a low hardness grade possessing exceptional tensile strength, superior compression set, chemical re.. |
|||
Middle Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 4455 Thermoplastic Elastomer A NSF certified, highly engineered Thermoplastic Elastomer for use in demanding applications. Sarlink® 4455 is a low hardness grade possessing exceptional tensile strength, superior compression s.. |
|||
Middle Barrel Temperature | 180 - 210 °C | 356 - 410 °F | cylinder |
Borealis BorSafe™ ME3420 MDPE Compound for Pressure Pipes BorSafe™ ME3420 is a bimodal polyethylene compound produced by the advanced Borstar® technology. Well dispersed carbon black gives outstanding UV resistance. Long term stability is ensured by an .. |
|||
Middle Barrel Temperature | 180 - 210 °C | 356 - 410 °F | |
Borealis RA130E Polypropylene Random Copolymer RA130E is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is natural colored. Applications RA130E is recommended for the production of PP-R pipes and .. |
|||
Middle Barrel Temperature | 180 - 210 °C | 356 - 410 °F | cylinder |
Borealis RA130E-2491 Polypropylene Random Copolymer RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISAKRIL® UNR ABS TISAKRIL has a wide area of application in automotive, electronics, computer, construction, and furniture industries. General Specifications include: High surface luminosityEasy processabilityDimens.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Mid-2. Region Temperature |
Tisan TISOPLEN® 40% Talc Filled Heat Stabilized Homopolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Middle Barrel Temperature | 196 - 210 °C | 385 - 410 °F | |
ExxonMobil Santoprene® 8201-90 Thermoplastic Elastomer A hard, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a w.. |
|||
Middle Barrel Temperature | 199 - 210 °C | 390 - 410 °F | |
Advanced Polymer Alloys DuraGrip™ DGR 6040 NC/BK Thermoplastic Elastomer (TPE) DuraGrip® DGR 6040 NC/BK are designed to be general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6040 NC/BK have
an excellent soft t.. |
|||
Middle Barrel Temperature | 190 - 210 °C | 374 - 410 °F | Injection Molding |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |
|||
Middle Barrel Temperature | 188 - 210 °C | 370 - 410 °F | Extrusion Metering Zone |
Teknor Apex Sarlink® 3150 Thermoplastic Elastomer A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3150 can be processed by injection molding or extrusion for appl.. |