Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G10 Polycarbonate, 10% Glass Reinforced Polycarbonate, 10% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G10-[color]-1 Polycarbonate, 10% Glass Reinforced with Mold Release Polycarbonate, 10% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G15 Polycarbonate, 15% Glass Reinforced Polycarbonate, 15% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polym.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G20 Polycarbonate, 20% Glass Reinforced Polycarbonate, 20% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G20-[color]-1 Polycarbonate, 20% Glass Reinforced with Mold Release Polycarbonate, 20% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G20-[color]-WS Polycarbonate, 20% Glass Reinforced Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G30 Polycarbonate, 30% Glass Reinforced Polycarbonate, 30% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G40 Polycarbonate, 40% Glass Reinforced Polycarbonate, 40% Glass ReinforcedFeatures: • Flame Retardant • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-p.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G40-[color]-1 Polycarbonate, 40% Glass Reinforced with Mold Release Polycarbonate, 40% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR1 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR1-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR1-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR1-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR2-[color]-1 Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR2-[color]-4 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold Release Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pig.. |
|||
Middle Barrel Temperature | 304 - 316 °C | 579 - 601 °F | |
LNP NORYL® EXCP0111 PPS + Polyphenylene Ether, 42% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Middle Barrel Temperature | 304 - 316 °C | 579 - 601 °F | |
LNP NORYL® EXCP0112 PPS + Polyphenylene Ether, 40% Glass / Mineral Reinforcement
(discontinued **) For applications requiring voltage resistance.Features: Corona resistantForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labele.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-G30-[color]-1 Polycarbonate, 30% Glass Reinforced with Mold Release Polycarbonate, 30% Glass Reinforced with Mold ReleaseProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR1-[color]-TFE Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear Resistant Polycarbonate, 10% Glass Reinforced, PTFE, Flame Retardant, Wear ResistantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR2 Polycarbonate, 10% Glass Reinforced, Flame Retardant Polycarbonate, 10% Glass Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PC-HM-FR2-[color]-3 Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilized Polycarbonate, 10% Glass Reinforced, Flame Retardant, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sampl.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® PCGF120 Polycarbonate, 20% Glass-Filled 20% glass-filled grade, good balance of impact and mechanical propertiesAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
LTL Color Compounds ColorFast® PCGF130 Polycarbonate, 30% Glass-Filled 30% glass-filled grade polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Middle Barrel Temperature | 304 - 321 °C | 579 - 610 °F | |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 304 - 321 °C | 579 - 610 °F | |
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 304 - 321 °C | 579 - 610 °F | |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Middle Barrel Temperature | 304 - 321 °C | 579 - 610 °F | |
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Middle Barrel Temperature | 304 - 321 °C | 579 - 610 °F | |
A. Schulman ComAlloy Lubrilon® 512 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Middle Barrel Temperature | 304 - 327 °C | 580 - 620 °F | |
Polymer Resources PCSF-FRG20 Polycarbonate, 20% Glass Reinforced Structural Foam Grade Polycarbonate, 20% Glass Reinforced Structural Foam GradeFeatures: • Flame Retardant • Foamable • Self ExtinguishingProcess: Foam MoldingNotes: All physical, mechanical and thermal testing con.. |