Processing Properties | Metric | English | Comments |
---|---|---|---|
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F36-01 35% Mica Reinforced Polypropylene Copolymer, Black Applications: Cowl screensHVAC ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT5250-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT5250-650UV Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products FT5250-650UVA Thermoplastic Polyolefin, UV Stabilized, Exterior 848 Black Applications: Cowl vent grillesExterior componentsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products GC30P104-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 232 °C | 410 - 450 °F | |
PlastiComp Complet® LGF30 - TPU Rigid Thermoplastic Polyurethane, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 30% long glass fiber reinforcementInformation provided by Plas.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | Zone 2; Cylinder |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Middle Barrel Temperature | 210 - 238 °C | 410 - 460 °F | |
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Middle Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | |
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | |
Multibase Multi-Flex® A 7727 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good .. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | |
Multibase Multi-Flex® D 2010 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good F.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | |
Multibase Multi-Flex® D 3604 TPE Thermoplastic Elastomer Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P.. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | H2 |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | H2 |
Samsung Cheil Industries Starex® WR-9750 Extrusion Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Middle Barrel Temperature | 210 °C | 410 °F | Cast film |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | Cast film |
DuPont Elvaloy® 3217 AC Ethylene and 17% Butyl Acrylate Copolymer Elvaloy® 3217 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3217 AC has been developed for film applications requiring a combination of softness, toughness and low friction. Typi.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | |
Beijing Chemical Industry KAIFA® GL3300 ABS Flame-Retardant Grade Good flammabilityInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Middle Barrel Temperature | 210 °C | 410 °F | |
Beijing Chemical Industry KAIFA® GL5200 ABS Extrusion Grade Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Middle Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Middle Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Tube Extrusion |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Middle Barrel Temperature | 210 - 230 °C | 410 - 446 °F | Injection Molding |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Middle Barrel Temperature | 210 °C | 410 °F | Cast film |
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
(discontinued **) Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill.. |