Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
50%; Recommended for 1/8" dia bead |
Parker Chomerics Tecknit® 72-00152 Silver-Filled Flexible Resin Caulking System Description: TECKNIT standard electrically conductive caulks consist of four one-component resin systems filled with silver plated glass or copper particles. These systems are formulated to provide .. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
|
Parker Chomerics THERM-A-FORM T644 Cure-in-Place Potting and Underfill Material Description: THERM-A-FORM™ thermally conductive silicone elastomer products are dispensable form-in-place compounds designed for heat transfer without excessive compressive force in electronics co.. |
|||
Cure Time | 4320 - 7200 min @Temperature 25.0 °C |
72.0 - 120 hour @Temperature 77.0 °F |
Complete Cure Cycle |
Northstar Polymers MCP-V40A Polyurethane Gel MCP-V40A is a polyurethane gel formulation specifically designed for padding and cushioning applications, where low rebound property of the material is critical. This viscoelastic polymer is a two.. |
|||
Cure Time | 4320 - 7200 min @Temperature 25.0 °C |
72.0 - 120 hour @Temperature 77.0 °F |
Complete Cure Cycle |
Northstar Polymers MPC-W44A Polyurethane Gel MPC-W44A is a polyurethane gel formulation specifically designed for padding and cushioning application that requires Shore Durometer OOO scale hardness. Produces good rebound characteristics and g.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
Aluminum, working strength |
Permabond HH131 High Temperature Threadlocker Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for .. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
Aluminum, working strength |
Permabond HH190 Anaerobic Gasketmaker Permabond® HH190 Gasketmaker is an anaerobic curing flange sealant that can replace, or be used as a dressing for, conventional pre-cut gaskets. Since HH190 is a flowable paste, it conforms to the .. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
Zinc, working strength |
Permabond HM128 Anaerobic Threadlocker Permabond® HM128 Threadlocker is a high strength adhesive for permanent assembly. It is typically used for preventing vibration loosening of bolts, studs and cap screws. Full cure to a cross-linked.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
Zinc, full strength |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
M10 steel, full strength |
Permabond LH050P Pure Anaerobic Threadsealant PERMABOND® LH050 PURE anaerobic pipe sealant is single component paste that cures only when in contact with metal parts and oxygen is excluded. The sealant fills up the entire space between male an.. |
|||
Cure Time | 4320 - 5760 min @Temperature 25.0 °C |
72.0 - 96.0 hour @Temperature 77.0 °F |
Complete Cure Cycle |
Northstar Polymers MPG-A25A Room-Temperature Curable Liquid Castable Polyurethane MPG-A25A is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott.. |
|||
Cure Time | 4320 - 5760 min @Temperature 25.0 °C |
72.0 - 96.0 hour @Temperature 77.0 °F |
Complete Cure Cycle |
Northstar Polymers SAI-1 Low Viscosity Variable Ratio Polyurethane Gel SAI-1 is custom formulated polyurethane gel material to yield very soft elastomer gel material from low viscosity components at room temperature. This material is variable mixing ratio so that the .. |
|||
Cure Time | 4320 - 18000 min @Temperature 23.9 °C |
72.0 - 300 hour @Temperature 75.0 °F |
|
Master Bond EP21LVSP6 Two component epoxy for bonding, sealing, coating and encapsulating Product Description: Master Bond EP21LVSP6 is a two component epoxy compound for high performance bonding, coating, sealing and encapsulating. It is formulated to cure at room temperature or more ra.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond FDA16 Food and Drug Application Epoxy Adhesive TRA-BOND FDA-16 EPOXY ADHESIVE is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests,.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond FS152C Clear Low Viscosity Epoxy Adhesive TRA-BOND FS152C is a low viscosity epoxy system containing no solvents, cures at room temperature and has excellent flow and wetting characteristics. This two-part adhesive mixes easily and develops.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond 216E01 Non-Sag Dam Applications Adhesive TRA-BOND 216E01 is a thixotropic, two-part adhesive formulated specifically for applications where a high-fill, non-sag adhesive is required. TRA-BOND 216E01 works in concert with TRA-BOND 216E02 to.. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Tra-Con Tra-Bond FDA12WH01 Food and Drug Application Epoxy Adhesive TRA-BOND FDA12 WH01 is a medium viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug .. |
|||
Cure Time | 4320 min @Temperature 10.0 °C |
72.0 hour @Temperature 50.0 °F |
Full Load |
Chesterton ARC 897 Fine Grade Sliding Wear Compound Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t.. |
|||
Cure Time | 4320 min @Temperature 16.0 °C |
72.0 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton ARC 897 Fine Grade Sliding Wear Compound Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t.. |
|||
Cure Time | 4320 min @Temperature 16.0 °C |
72.0 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton ARC I BX1 Impact & Wear Resistant Epoxy Composite Description: An advanced grade epoxy and urethane composite for the repair and protection of all metal surfaces subjected to severe abrasion and impact. It is normally applied at a thickness of 6 mm.. |
|||
Cure Time | 4320 min @Temperature 32.0 °C |
72.0 hour @Temperature 89.6 °F |
Full Mechanical/Chemical |
Chesterton ARC MXHT High temperature severe wear compound Description: An advanced ceramic composite for the protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack at elevated temperatures. It is applied at a thickness o.. |
|||
Cure Time | 4320 - 7200 min @Temperature 25.0 °C |
72.0 - 120 hour @Temperature 77.0 °F |
|
Cytec Conathane® CE-1175 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
|
Epoxy Technology EPO-TEK® 301-2FL Low Stress, Optical Epoxy Product Description: EPO-TEK® 301-2FL is a two component optical, medical, and semiconductor grade epoxy resin. It is a more flexible version of EPO-TEK® 301-2.Advantages & Application Notes: Sug.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
|
Epoxy Technology EPO-TEK® EJ2189 Electrically Conductive Epoxy Product Description: EPO-TEK® EJ2189 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although othe.. |
|||
Cure Time | 4320 min @Temperature 23.0 °C |
72.0 hour @Temperature 73.4 °F |
|
Epoxy Technology EPO-TEK® EJ2189-LV Electrically Conductive Epoxy Low Viscosity, two component room temp curing conductive epoxyInformation Provided by Epoxy Technology |
|||
Cure Time | 4320 min @Temperature 32.0 °C |
72.0 hour @Temperature 89.6 °F |
Full Mechanical |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Cure Time | 4320 min @Temperature 32.0 °C |
72.0 hour @Temperature 89.6 °F |
Full Chemical |
Chesterton ARC HT-S High Temperature Corrosion Resistant Coating Description: ARC HT-S is a high temperature corrosion resistant coating for continuous operating conditions at elevated temperatures. It is easily applied by brush or roller and can be sprayed with .. |
|||
Cure Time | 4320 min @Temperature 25.0 °C |
72.0 hour @Temperature 77.0 °F |
|
Atom Adhesives AA-BOND FDA16 Epoxy Adhesive AA-BOND FDA16 is a medium viscosity epoxy resin system specifically developed for medical device applications. AA-BOND FDA16 has been tested in accordance with USP biological reactivity tests, in vi.. |
|||
Cure Time | 4320 - 7200 min @Temperature 24.0 °C |
72.0 - 120 hour @Temperature 75.2 °F |
full cure |
BCC Products BC 8675E Polyurethane Elastomer BC 8675E is a multi-purpose elastomer that can perform many functions. Typical product features are: easy to use, cures at room temperature, resists moisture absorption, excellent in use for molds f.. |
|||
Cure Time | 4320 min @Temperature 16.0 °C |
72.0 hour @Temperature 60.8 °F |
Full Chemical |
Chesterton MRS 58 Metal Rebuilding System An advanced ceramic composite for the repair and protection of all metal surfaces subjected to erosion, corrosion and chemical attack. It is normally applied at a thickness of 1.5 mm (60 mils) or mo.. |