Processing Properties | Metric | English | Comments |
---|---|---|---|
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond F202 Anaerobic Retainer The unique 'toughening' process incorporated into Permabond® F202 gives this anaerobic adhesive excellent resistance to peel and impact forces. Primarily designed for use on metal surfaces, it is a.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HH120 Anaerobic Threadlocker Permabond® HH120 Threadlocker is an excellent general purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Its high viscosity allows for .. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Zinc, handling strength |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HM118 Anaerobic Threadlocker Permabond® HM118 Threadlocker is an excellent general-purpose threadlocker and sealant. It is used for locking bolts, nuts and screws that require permanent assembly. Cure is fast and reliable on s.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HM160 Anaerobic Retaining Compound Permabond® HM160 is a medium viscosity liquid adhesive that cures when confined between metal parts to form a tough, hard plastic. In the uncured, liquid state, the adhesive wets the metal surfaces.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HM161 Anaerobic Retaining Compound Permabond® HM161 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space’ between parts and upon cure unitiz.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HM162 Anaerobic Retainer Permabond® HM162 is a medium viscosity retaining compound that cures when confined between metal parts to form an extremely tough bond. It is best suited for cylindrical parts and where high temper.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HM163 Anaerobic Retainer Permabond® HM163 is a medium viscosity, thixotropic anaerobic retaining compound that cures when confined between metal parts to form a tough bond. It has been specifically formulated to provide a .. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond F201 Anaerobic Retainer Permabond® F201 is an anaerobic adhesive which has been developed to give excellent resistance to peel and impact forces. This toughening, combined with good adhesion to aluminum and copper alloys,.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HH040 Pure NSF 61 Approved Anaerobic Retainer Permabond® HH040 PURE is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure u.. |
|||
Cure Time | 4.98 - 9.60 min @Temperature 149 °C |
0.0830 - 0.160 hour @Temperature 300 °F |
|
Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and.. |
|||
Cure Time | 4.98 - 10.0 min @Temperature 149 °C |
0.0830 - 0.167 hour @Temperature 300 °F |
|
Master Bond Supreme 3HTND-1SM Fast Curing, One Component, Surface Mount Adhesive Master Bond Polymer System Supreme 3HTND-1SM is a one component, exceptionally fast curing surface mount adhesive system with exceptional toughness and durability. It has high shear and peel strengt.. |
|||
Cure Time | 4.98 - 10.0 min @Temperature 149 °C |
0.0830 - 0.167 hour @Temperature 300 °F |
|
Master Bond Supreme 3HTND-2GT One Part, Toughened, Fast Curing Glob Top Adhesive Master Bond Polymer System Supreme 3HTND-2GT is a fast curing, toughened one component high performance epoxy adhesive/sealant which meets the growing need for precise positioning and bonding of mic.. |
|||
Cure Time | 4.98 - 9.60 min @Temperature 149 °C |
0.0830 - 0.160 hour @Temperature 300 °F |
|
Master Bond EP3HT Fast Curing One Component Epoxy System Master Bond Polymer System EP3HT is a one component system featuring high shear strength and good temperature resistance along with a fast cure schedule. Master Bond Polymer System EP3HT produces du.. |
|||
Cure Time | 4.98 - 9.60 min @Temperature 149 °C |
0.0830 - 0.160 hour @Temperature 300 °F |
|
Master Bond EP3HTMED One Component, Biocompatible Epoxy System Master Bond Polymer System EP3HTMed combines the ease of a one part, no mix, fast curing adhesive with high shear strength. This special formulation fully meets USP Class VI requirements. EP3HTMed p.. |
|||
Cure Time | 4.98 min @Temperature 43.0 °C |
0.0830 hour @Temperature 109 °F |
Tack Free |
Chesterton ARC MX5 Rapid Curing Fine Particle Wear Compound Description: An advanced ceramic reinforced composite for the emergency repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a th.. |
|||
Cure Time | 4.98 min @Temperature 75.0 °C |
0.0830 hour @Temperature 167 °F |
Dust Free, at 50% humidity |
Blue River Coatings Semi-Transparent Wood Stain Concentrate BLUE RIVER COATINGS Semi-Transparent Wood Stain is a water based stain developed to provide long lasting protection and a beautiful appearance on wood surfaces. BLUE RIVER COATINGS Semi-Transparent .. |
|||
Cure Time | 4.98 min @Temperature 75.0 °C |
0.0830 hour @Temperature 167 °F |
Recoat, at 50% humidity |
Blue River Coatings Semi-Transparent Wood Stain Concentrate BLUE RIVER COATINGS Semi-Transparent Wood Stain is a water based stain developed to provide long lasting protection and a beautiful appearance on wood surfaces. BLUE RIVER COATINGS Semi-Transparent .. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond A1044 Anaerobic Threadsealant Permabond® A1044 is a rapid curing sealant designed to lock and seal metal pipe connections, offering very good resistance to even the most aggressive chemicals. Permabond A1044 can be used to seal.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond HM135 Anaerobic Retainer Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras.. |
|||
Cure Time | 4.98 - 10.2 min @Temperature 23.0 °C |
0.0830 - 0.170 hour @Temperature 73.4 °F |
M10 steel, handling strength |
Permabond HM135 Anaerobic Retainer Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond A113 Anaerobic Threadlocker Designed for the locking and sealing of metal parts, Permabond® A113 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used .. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |
|||
Cure Time | 4.98 min @Temperature 23.0 °C |
0.0830 hour @Temperature 73.4 °F |
Brass, handling strength |
Permabond A130 Anaerobic Threadlocker Designed for the locking and sealing of metal parts, Permabond® A130 is ideally suited for use on components that need to be dismantled for maintenance. Giving vibration resistance it can be used t.. |
|||
Cure Time | 4.98 min @Temperature 75.0 °C |
0.0830 hour @Temperature 167 °F |
Dust Free, at 50% humidity |
Blue River Coatings Acrylic 4000 Topcoat BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT is a hard, flexible, economical coating designed for multiple substrates. BLUE RIVER COATINGS ACRYLIC 4000 TOPCOAT offers good application properties, low fo.. |