Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Master Bond EP3HT Fast Curing One Component Epoxy System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Master Bond Inc.
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Master Bond EP3HT Fast Curing One Component Epoxy System.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Master Bond Polymer System EP3HT is a one component system featuring high shear strength and good temperature resistance along with a fast cure schedule. Master Bond Polymer System EP3HT produces durable, high strength bonds which are remarkably resistant to severe thermal cycling and many chemicals including water, oil, fuels and most organic solvents even upon prolonged exposures.
Physical Properties Metric English Comments
Viscosity >= 250000 cP

@Temperature 23.0 °C
>= 250000 cP

@Temperature 73.4 °F
Storage Temperature 23.9 °C
75.0 °F
6 months
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Processing Properties Metric English Comments
Cure Time 4.98 - 9.60 min

@Temperature 149 °C
0.0830 - 0.160 hour

@Temperature 300 °F
19.8 - 30.0 min

@Temperature 121 °C
0.330 - 0.500 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Color Yellow to Brown