Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 285 - 300 °C | 545 - 572 °F | |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Zone 4 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S31 (3484) PA 6.10 Dry
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 4 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF 30 4 (3552) PA 6.10 Dry, 30% Glass Filled
(discontinued **) A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 25 (2420) PA 6.6 Dry, 25% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 260 - 300 °C | 500 - 572 °F | |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Dry, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 20 (2470) PA 6 Dry, 20% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 9 RM-M (3099) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 (2475) PA 6 Dry, 50% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 4 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 4 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF 23 1 (2917) PA 6.10 Dry, 23% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 4 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF 30 1 (3222) PA 6.10 Dry, 30% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 4 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |
|||
Zone 4 | 220 - 300 °C | 428 - 572 °F | |
Akro-Plastic Akromid® S3 GF15 1 (3223) PA 6.10 Dry, 15% Glass Filled A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia.. |