Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 4 | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Zone 4 | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Zone 4 | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Zone 4 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 5300 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5300 is a static dissipative thermoplastic compound based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance valu.. |
|||
Zone 4 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 4 | 210 °C | 410 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 4 | 210 °C | 410 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val.. |
|||
Zone 4 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Zone 4 | 210 °C | 410 °F | Cylinder |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Zone 4 | 210 °C | 410 °F | Die |
Premix Thermoplastics PRE-ELEC® TPE 1502 Conductive Thermoplastic Compound PRE-ELEC® TPE 1502 is a conductive thermoplastic compound based on a thermoplastic elastomer (TPE). Conductivity is achieved by using a special conductive carbon black. In addition to a low electri.. |
|||
Zone 4 | 210 - 230 °C | 410 - 446 °F | Extrusion Molding |
LG Chemical LI970 Co-Extrusion ASA Description: Good Weatherability, Scratch ResistanceApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Zone 4 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® ECO 12T95 Thermoplastic Polyurethane Type : Pearlthane® ECO 12T95 is a high performance bio-based thermoplastic polyurethane. With ca. 32% bio-based content.Main Application : Injection MouldingSpecial Features : Excellent mechanica.. |
|||
Zone 4 | 210 - 220 °C | 410 - 428 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D12T90E Thermoplastic Polyurethane PEARLTHANE® ECO D12T90E is a 91 Shore A, High Performance natural TPU based on Renewable Sources with ca. 37% renewable content according to ASTM D6866 for Extrusion and Blow moulding application.. |
|||
Zone 4 | 210 °C | 410 °F | Injection Molding |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Zone 4 | 210 °C | 410 °F | Extrusion |
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket.. |
|||
Zone 4 | 210 - 220 °C | 410 - 428 °F | Injection |
Lubrizol ESTANE® GP98AE Ester Based Thermoplastic Polyurethane Type: Estane® GP 98AE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided b.. |
|||
Zone 4 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Appeel® 72D811 Sealing Resin DuPont™ Appeel® 72D811 resin is designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDPE, LDPE, EVA, and Ion.. |
|||
Zone 4 | 210 °C | 410 °F | Blown Film Coextrusion |
DuPont™ Bynel® 22E780 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Zone 4 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Elvax® 3128-1 Ethylene Vinyl Acetate DuPont™ Elvax® 3128-1 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® .. |
|||
Zone 4 | 210 °C | 410 °F | Cast Film/Sheet Processing |
DuPont™ Surlyn® E185SB Ionomer Resin Surlyn® E185SB is an ionomer of an acid copolymer resin. It is designed for coextrusion with high-density polyethylene in peelable seals applications. It can be used in extrusion equipment designed.. |
|||
Zone 4 | 210 °C | 410 °F | Extrusion Coating |
DuPont™ Elvaloy® AC 15024S Ethylene Methyl Acrylate Elvaloy® AC 15024S is a copolymer of ethylene and methyl acrylate. It is available in pellet form for use in conventional extrusion equipment designed to process polyethylene type resins. Elvaloy®.. |
|||
Zone 4 | 210 - 230 °C | 410 - 446 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Zone 4 | 210 - 230 °C | 410 - 446 °F | |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||
Zone 4 | 210 °C | 410 °F | Nozzle |
BASF Ultraform® N2200 G43 POM Description: Is a POM, injection-molding grade for parts requiring high stiffness and strength together with good mold release.Information provided by BASF |
|||
Zone 4 | 210 °C | 410 °F | Nozzle |
BASF Ultraform® N2720 M63 30% Mineral Filled POM Description: Is a POM, 30 % mineral-reinforced material for low-warpage moldings with high stiffness, strength and hardness.Information provided by BASF |
|||
Zone 4 | 210 °C | 410 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T93 Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T93 is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining hardness with excellent mechanical prop.. |