| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Zone 4 | 215 - 235 °C | 419 - 455 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 4 | 215 - 235 °C | 419 - 455 °F | Extrusion Molding |
| LG Chemical KEYFLEX BT 3038D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® EG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® EM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® GP Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® IG Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 210 - 235 °C | 410 - 455 °F | Vent; Extrusion |
| Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
| Zone 4 | 225 - 235 °C | 437 - 455 °F | Injection |
| Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||