Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 1200-8493 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 65-7311 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 65-8285 PP-copolymer, with carbon fiber Applications: Office communication.High-stiff parts with low creep.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided b.. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 65-8378 PP-copolymer, with carbon fiber Applications: Office communication.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Low warpage.Information provided by Lehmann & .. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 65-8452-1 PP-copolymer, with aramid reinforcement, lubricant modified Applications: Office communication.Low warpage, isotropic shrinkage characteristics.Dynamic stressed parts.Information provided by Lehmann & Voss & Co.KG |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 65-8498 PP-copolymer, unreinforced Applications: Office communication.Reduced moment of inertia compared with metal parts.Dynamic stressed parts.Especially suitable for thin wall complex parts.Information provided by Lehmann & Voss &.. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 1200-7899 ABS, with steel fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Isotropic shrinkage characteristics.Information provided by Lehman.. |
|||
Zone 3 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide B28 PA6, Injection Molded Staramide B28 is an Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide B28N PA6, Nucleated, Injection Molded Staramide B28N is a Nucleated and Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide BG2ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG2ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar. |
|||
Zone 3 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Staramide PF007IX2 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF007IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as Star X 2010 33V)Information provided by Eurostar. |
|||
Zone 3 | 250 - 260 °C | 482 - 500 °F | |
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Star L PA6 D61 PA6, Injection Molded Star L PA6 D61 is a PTFE/Silicone Oil Lubricated, Unreinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 240 - 260 °C | 464 - 500 °F | |
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 230 - 260 °C | 446 - 500 °F | |
Lehmann & Voss LUVOCOM® 1200-7116-2 ABS, with carbon fiber Applications: Office communication.Reduced moment of inertia compared with metal parts.Electrically conductive, suitable for continuous discharging of statically generated electricity.Strong, stiff .. |