Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7004 Polyamide 66, with glass fiber and carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8064 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/CF/20/HS Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/CF/30/TF/13/SI/2/BK Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-0866 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-0935 Polyamide 66, with glass fiber and PTFE, 8-mm-granulate Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-1119 VP Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7032-B Polyamide 66, with aramid reinforcement and PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Improved heat resistance.Control disks, cams, sliding elem.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7360/EG Polyamide 66, with PTFE, lubricant modified, high viscosity, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property.Bea.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7817 Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrical.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7893/GY Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/CF/10/TF/20/BK Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Electrically conductive, suita.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/XCF/25 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-0890 Polyamide 66, with carbon fiber, low-warpage, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Stiff parts, low coefficient of expansion, low viscose, anisotropic.Reduced moment of inertia c.. |
|||
Zone 3 | 270 - 310 °C | 518 - 590 °F | |
Topas Advanced Polymers TOPAS® 6017S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6017S-04 is an injection molding grade with a high heat distortion temperature (170°C) and exceptional dimensional stability. It is a glass-clear amorphous polymer with outstanding moisture.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |
|||
Zone 3 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |