Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 3 | 225 - 245 °C | 437 - 473 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1063D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 3 | 225 - 245 °C | 437 - 473 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Zone 3 | 225 °C | 437 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T60D Thermoplastic Polyurethane Elastomer Type : Pearlthane® 11T60D is a polycaprolactone copolyester-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Combining very high hardness with excellent me.. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HU 70E3 HDPE, Injection Molding Starpylen HU 70E3 is a High Density Polypropylene Injection Molding Resin (also known as HU70E3)Information provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MF003SU PP, 15% Glass Fiber Filled, Injection Molded Starpylen MF003SU is a 15% Glass Fiber Reinforced Polypropylene Injection Molding Resin (also known as Starpylen WX 15V S34/040)Information provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MF007AS PP, Glass Fiber Filled, Injection Molded Starpylen MF007AS is a Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MF008S PP, 40% Glass Fiber Filled, Injection Molded Starpylen MF008S is a 40% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MFM43S PP, Glass/Mineral Filled, Injection Molded Starpylen MFM43S is a Mineral Filled, Glass Fiber Reinforced, Polypropylene Injection Molding Resin, also recognized as Starpylen WV 30VMC S37/7 Black 301Information provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MH0200A HDPE, Injection Molding Starpylen MH0200A is a High Density Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MK001AS PP, Mineral Filled, Injection Molding Starpylen MK001AS is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MX06023 PP, 20% Milled Glass Fiber Filled, Injection Molded Starpylen MX06023 is a 20% Milled Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 250 °C | 437 - 482 °F | |
Eurostar Starpylen MX06050 PP, 30% Glass Filled, Injection Molded Starpylen MX06050 is a 30% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 RM-M (3146) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 60 (2476) PA 6 Dry, 60% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 °C | 437 °F | Extrusion |
Alliance Polymers Zythane™ 7065D Thermoplastic Polyurethane Elastomer Zythane™ 7065D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Zone 3 | 225 - 245 °C | 437 - 473 °F | Front |
BASF Ultramid® HFX 33 PA6 (Dry) Description: Ultramid HFX 33 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 3 | 225 - 245 °C | 437 - 473 °F | Front |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Zone 3 | 225 - 245 °C | 437 - 473 °F | Front |
BASF Ultramid® HFX 37 PA6 (Dry) Description: Ultramid HFX 37 is a polyamide specialty extrusion resin combining high flexibility, excellent burst performance and outstanding chemical resistance. It offers high melt strength and en.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 (2500) PA 6 Dry AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 15 (2469) PA 6 Dry, 15% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 30 RM-M (3016) PA 6 Dry, 30% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 35 (2473) PA 6 Dry, 35% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 40 (2474) PA 6 Dry, 40% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
Zone 3 | 225 - 300 °C | 437 - 572 °F | |
Akro-Plastic Akromid® B3 GF 50 9 RM-M (3147) PA 6 Dry, 50% Glass Filled In all, the construction relevant features show that the significantly reduced moisture absorption of AKROMID B3 GF 30 RM leads to increasing rigidities and strengths as already expected. Neverthele.. |