Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7198/BK PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7741 PEEK, with mineral filler, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7766 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7809/BK PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8099 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Reduced moment of inertia compared with metal parts.Chemical and hydrolysis resistance par.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8108 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.Improved frict.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8382 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Highly dimensionally stable at ele.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8417 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 2 | 340 - 390 °C | 644 - 734 °F | |
Lehmann & Voss LUVOCOM® 1106/XCF/30 Polyether imide, with carbon fiber, easy flowing Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Electrically conductive, suitable for continuous dis.. |
|||
Zone 2 | 340 - 390 °C | 644 - 734 °F | |
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical.. |
|||
Zone 2 | 340 - 390 °C | 644 - 734 °F | |
Lehmann & Voss LUVOCOM® 1106-8089/BL Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® TPI-0953 Thermoplastic polyimide, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, apparatus- and precision engineering medical- and electrical enineering, aircraft- and aerospace industry.Very high continuous use and heat dist.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105/BK0873 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Especially suitable for medical parts, super.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105/XCF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7106 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7596/BL PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7714 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts,.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7826/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 2 | 340 - 390 °C | 644 - 734 °F | |
Lehmann & Voss LUVOCOM® 1106-7223 Polyether imide, with PTFE Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 2 | 340 - 390 °C | 644 - 734 °F | |
Lehmann & Voss LUVOCOM® 1106-8232 Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105/CF/15 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 2 | 335 - 390 °C | 635 - 734 °F | |
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU) Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® 1105-7825 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Zone 2 | 380 - 390 °C | 716 - 734 °F | |
Lehmann & Voss LUVOCOM® PEEK CLASSIX 7918 PEEK, unreinforced Applications: medical engineeringEspecially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical resistance parts, non flammable.Inherent flame resistance.S.. |