Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7305/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7395 Polyamide 66, with carbon fiber, aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved wear behaviour, low warpage.Emergency running property, for highest tribologic needs.R.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-7805 Polyamide 66, with glass fiber, aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8070 VP Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8379 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1-8501 Polyamide 66, with glass fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.dynamic st.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50/CF/10/GF/20/BK Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50/CF/20 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50/CF/7/GS/10/TF/5/EM/BK Polycarbonate, with carbon fiber, glass flakes and PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-0833 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Electrical.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7154/V0 Polycarbonate, with carbon fiber, low-warpage Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7164/BL02 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Low warpag.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7224/V0 Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Reduced moment of inertia compared with metal parts.Improved f.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7228 Polycarbonate, with carbon fiber, glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Electrically conductive, suitable for cont.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7446 Polycarbonate, with carbon fiber, PTFE, lubricant modified Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7807 Polycarbonate, with carbon fiber and demolding aid Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50-7814/EM Polycarbonate, with glass fiber and PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/CF/20 Polyamide 66, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 1/TF/18/SI/2/BK Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOCOM® 50/CF/5/GF/10 Polycarbonate, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High-strength and high-stiff parts; low coefficient of expansi.. |
|||
Zone 2 | 290 - 310 °C | 554 - 590 °F | |
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |