Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80/TF/22/NT Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-0837-1 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7014 Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7112/BK Polyacetal-copolymer, with glass fiber and carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7353/NAT Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7388 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7555 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7580 Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7653 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Antistatic.No change of electric potential at bearings in case of separation of charge caused b.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7655/RD Polyacetal-copolymer, with aramid reinforcement and PTFE, toughness-modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7713-NA Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-7917 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-8268 Polyacetal-copolymer, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-8284 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-8387/EM Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Strong, stiff parts.Impact resistance.Control disks, cams, .. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-8510 Polyacetal-copolymer, with mineral filler, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-8511 Polyacetal-copolymer, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.High dimensionally.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | Injection Molding |
Kolon ELLAS K-793AB Ester Based Thermoplastic Polyurethane ApplicationsFilm/SeatBlown filmIndustry Parts Information provided by API-Kolon. |
|||
Zone 1 | 170 - 190 °C | 338 - 374 °F | |
Lubrizol Advanced Materials Pearlthane® Clear 15N70 Polyether based TPU PEARLTHANE® CLEAR 15N70 is a polyether copolymer-based TPU with Shore 72 A hardness, free of plasticizer, supplied in form of translucent, colorless pellets with very low yellowness index. PEARLT.. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® 80-8003 Polyacetal-copolymer, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Electrically conductive, suitable for continuous discharging of statically .. |
|||
Zone 1 | 175 - 190 °C | 347 - 374 °F | |
Lehmann & Voss LUVOCOM® AC-80/TF/22/BK Polyacetal-copolymer, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam M10009A PP, Flame Retardant, Injection Molding Starflam M10009A is an Unfilled Flame Retardant Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam M10009AP PP, Flame Retardant, Injection Molding Starflam M10009AP is an Unfilled Flame Retardant high fluidity Polypropylene (Homo) Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 180 - 190 °C | 356 - 374 °F | |
Eurostar Starflam MX05075 PP, Flame Retardant, Injection Molding Starflam MX05075 is an Unfilled Halogen Free Flame Retardant PP Injection Molding ResinInformation provided by Eurostar. |
|||
Zone 1 | 170 - 190 °C | 338 - 374 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1035D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |