Processing Properties | Metric | English | Comments |
---|---|---|---|
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7185 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7194/GY PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7301 PEEK, unreinforced, laser markable Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7905 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7907 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7944 PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Emergency running property.High chemical resistance parts, hydrolysis resistance, non flam.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8065 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8102 PEEK, with PTFE, lubricant modified, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8157 PEEK, with CNT Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8234 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Dynam.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8354 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8432 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8513 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1502-7866/GN4 PPSU, unreinforced Applications: Automotive industry, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceHigh chemical res.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/BK7308-1 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0797 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0948/YL2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7685 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Super.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7709/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8184 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-8389/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105/XCF/30 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Zone 1 | 360 - 370 °C | 680 - 698 °F | |
Lehmann & Voss LUVOCOM® 1105-7173/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |