Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® ABS 1410 PRE-ELEC ABS 1410 is a conductive thermoplastic compound based on ABS. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC ABS 141.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PE 1291 PRE-ELEC PE 1291 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PE 1294 PRE-ELEC PE 1294 is a conductive thermoplastic compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELEC PE 129.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® PP 1386 PRE-ELEC PP 1386 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Die Temperature | 220 °C | 428 °F | Zone 3 |
Premix Thermoplastics PRE-ELEC® CP 1318
(discontinued **) PRE-ELEC CP 1318 is a conductive thermoplastic compound based on a polyolefin copolymer. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivit.. |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Average value: 238 °C Grade Count:6 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 220 - 260 °C | 428 - 500 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 2140D Ester Type TPE Description: Injection Molding, TPC-ET, Specialty, Low ModulusApplication: Films & SheetsCAS: 37282-12-5Information provided by LG Chemical |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® EH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | Extrusion |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Die Temperature | 220 - 230 °C | 428 - 446 °F | 6 |
Lubrizol Advanced Materials Pearlthane® ECO D12T55D Thermoplastic Polyurethane Type: Pearlthane® ECO D12T55D is a high performance bio-based thermoplastic polyurethane. With ca. 29% bio-based content.Main Application : Extrusion/MouldingSpecial Features : Properties similar.. |
|||
Die Temperature | 220 - 230 °C | 428 - 446 °F | |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Die Temperature | 220 °C | 428 °F | |
Borealis Borclear™ RC707MO Polypropylene Borclear™ RC707MO is intended for blow molding. This grade provides high gloss, high transparency and excellent impact properties. This grade also features high heat distortion temperature. Applic.. |
|||
Die Temperature | 220 °C | 428 °F | Blow Film |
DuPont Appeel® LSR11D542 Lidding Sealant Resin Appeel® LSR11D542 is a modified ethylene vinyl acetate copolymer resin designed to function as a peelable sealing layer for lidding and pouch applications. It provides a peelable seal and a "whiten.. |
|||
Die Temperature | 220 °C | 428 °F | Extrusion Coating |
DuPont™ Appeel® 11D888 Ethylene Vinyl Acetate Appeel®11D888 is a developmental modified ethylene vinyl acetate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a .. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18365-S Grafted Maleic Anhydride Polyethylene OREVAC 18365-S is a grafted maleic anhydride polyethylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC 18365-S is mainly used in multi-layer tube to have good adhesion between.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18510 Grafted Maleic Anhydride Polyethylene OREVAC 18510 is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510 is mainly used in pipe .. |
|||
Die Temperature | 220 °C | 428 °F | Extrusion |
Alliance Polymers Zythane™ 5050D Thermoplastic Polyurethane Elastomer Zythane™ 5050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Die Temperature | 220 °C | 428 °F | Extrusion |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® 18760 Grafted Maleic Anhydride Polypropylene OREVAC 18760 is a maleic anhydride grafted polypropylene used in the manufacturing of three layer PP coating for steel pipeline. OREVAC 18760 is also used in multilayer EVOH – PP structures. OREVAC.. |
|||
Die Temperature | 220 - 240 °C | 428 - 464 °F | |
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA.. |
|||
Die Temperature | 220 - 250 °C | 428 - 482 °F | Tube Extrusion |
Arkema Group KYNAR FLEX® 2750-01 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |