Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borclear™ RC707MO Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Borealis
Trade Name Borclear™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borclear™ RC707MO Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Borclear™ RC707MO is intended for blow molding. This grade provides high gloss, high transparency and excellent impact properties. This grade also features high heat distortion temperature. Applications: cosmetics, bottles for detergents and for the food industry.Information provided by Borealis AG
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min
3.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
50mm/min; ISO 527-2
Tensile Modulus 1.00 GPa
145 ksi
1mm/min; ISO 527-2
Charpy Impact, Notched 0.400 J/cm²

@Temperature 0.000 °C
1.90 ft-lb/in²

@Temperature 32.0 °F
ISO 179/1eA
1.50 J/cm²

@Temperature 23.0 °C
7.14 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ISO 75-2
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
bottle, 6mm thick; Borealis Method
15 %
15 %
2mm plaque; Borealis Method
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Middle Barrel Temperature 230 °C
446 °F
Die Temperature 220 °C
428 °F
Melt Temperature 230 °C
446 °F
Users viewing this material also viewed the following: