Processing Properties | Metric | English | Comments |
---|---|---|---|
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est.. |
|||
Die Temperature | 170 - 220 °C | 338 - 428 °F | |
Solvay Specialty Polymers Cogegum® GFR/340-HP Polyolefin, Unspecified
(Unverified Data**) Cogegum® XLPO-HFFR - Crosslinkable Halogen Free Fire Retardant compound Silane grafted compound moisture curable by addition of a catalyst masterbatch (Sioplas® method). It consists of a polyolefi.. |
|||
Die Temperature | 215 - 220 °C | 419 - 428 °F | |
Lubrizol Advanced Materials PEARLTHANE® 11T98 Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T98 is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, combining high hardness with excellent mechanical properties. It can be extruded.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1109 MD Chemically-Crosslinkable MDPE Compound TABOREX TA 1110 MD is a crosslinkable compound made by a Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOP.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1117HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1117 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | |
Silon Taborex TA 1135 HD Chemically-Crosslinkable HDPE Compound TABOREX TA 1135 HD is a crosslinkable compound made by Silane grafted ethylene polymer. This graft polymer constitutes together with a Masterbatch containing the crosslinking catalyst a “SIOPLA.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Extrusion |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL2571 High Density Polyethylene BL2571 is a high-density polyethylene with high stiffness and high environmental stress crack resistance. This product is intended for blow molding. Applications: household and chemical containers.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis BL2631 High Density Polyethylene BL2631 is a high density polyethylene homopolymer intended for blow molding of products requiring high toughness and stiffness. Applications: fresh milk bottles, and juice bottles.Information provi.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis Borcoat™ BB108E-1199 White Polypropylene Block Copolymer for Steel Pipe Coating Borcoat BB108E-1199, a ready made white compound, is a highly molecular weight, low melt flow polypropylene block copolymer. As a top-coat in three component polypropylene systems, Borcoat BB108E-1.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA2000 Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA2000 is a high molecular weight, low melt flow rate polypropylene block copolymer with a good balance of mechanical properties. This grade offers superior stiffness while keeping good im.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis BorECO™ BA415E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO™ BA415E is a high molecular weight, low melt flow rate polypropylene block copolymer with high stiffness and impact strength. This material has been designed for improved processability and.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-2491 Polypropylene Random Copolymer RA130E-2491 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is blue colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6017 Polypropylene Random Copolymer RA130E-6017 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-6034 Polypropylene Random Copolymer RA130E-6034 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is green colored. Applications: domestic water, heating, relining, plumbing, and indust.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-2492 Polypropylene Random Copolymer RA130E-2492 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is dark blue colored. Applications: domestic water, heating, relining, plumbing, and in.. |
|||
Die Temperature | 210 - 220 °C | 410 - 428 °F | |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis RB206MO Polypropylene Random Copolymer RB206MO is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade also .. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | |
Borealis RB607MO Polypropylene Random Copolymer RB607MO is a random copolymer for blow molding, with good transparency and contact clarity, very good gloss and surface finish. Bottles up to 2 liters can be steam sterilized due to heat distortion .. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | Hotmelt Coating Slot Die |
EMS-Griltech Griltex® D 1442E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Die Temperature | 190 - 220 °C | 374 - 428 °F | Average value: 205 °C Grade Count:18 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Die Temperature | 180 - 220 °C | 356 - 428 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 1035D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical |