Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 200 °C | 392 °F | |
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicati.. |
|||
Feed Temperature | 200 °C | 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Feed Temperature | 200 - 230 °C | 392 - 446 °F | |
Lavergne VYTEEN PC/ABS 3016 PC-ABS, 16% Glass Reinforced Vyteen PC/ABS 3016 is a black 16% glass fiber reinforced Polycarbonate/ABS alloy designed for injection molding.Features: -Good processability -Balanced stiffness/resilience -High deflection temp.. |
|||
Feed Temperature | 200 °C | 392 °F | |
Lubrizol Advanced Materials PEARLTHANE® D11H95S Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H95S is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring excellent flow and mechanical properties and an out.. |
|||
Feed Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-ED71 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Feed Temperature | 200 - 210 °C | 392 - 410 °F | |
Solvay TECHNYL® C 442 Black V PA6, DRY Description: Unreinforced polyamide PA6, high viscosity, with high flexibility and very high impact resistance even at low temperature, for extrusion.Available in: Europe Product Applications: It ha.. |
|||
Feed Temperature | 200 - 220 °C | 392 - 428 °F | |
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Feed Temperature | 200 - 220 °C | 392 - 428 °F | |
Solvay TECHNYL® C 536XT PA6, DRY Description: TECHNYL® C 536XT is an unreinforced polyamide 6, high viscosity, for extrusion blow molding. This product is available in natural color.Benefits: The product offers a good processing.. |
|||
Feed Temperature | 200 °C | 392 °F | |
Taiwan PU Corporation TPUI-T64D Transparent Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
Feed Temperature | 200 - 215 °C | 392 - 419 °F | |
Lubrizol Estane® S160D Thermoplastic Polyurethane Type: Estane® S160D is a Shore 63D, polyester based thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Americas, Europe, Middle East, .. |
|||
Feed Temperature | 200 - 215 °C | 392 - 419 °F | |
Lubrizol Estane® S360D Thermoplastic Polyurethane Type: Estane® S360D is a Shore 63D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |
|||
Feed Temperature | 200 - 215 °C | 392 - 419 °F | |
Lubrizol Estane® S364D Thermoplastic Polyurethane Type: Estane® S364D is a Shore 65D, polyester based thermoplastic polyurethane (TPU) with excellent transparency. FDA approved (21 CFR 177.2600, 177.1680).Uses: Injection Molding.Availability: Asi.. |