Processing Properties | Metric | English | Comments |
---|---|---|---|
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom for Electronic and Electric Standard Molding |
Mitsui Arlen™ A335 35% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom for Electronic and Electric Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ A350 50% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ C230 30% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom for Electronic and Electric Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (COND) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom Temp for Mechanical and Structural Standard Molding |
Mitsui Arlen™ CH230N 30% Glass Fiber-Reinforced Modified Nylon 6T, Flame Retardant (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB7 GR15 NL RT PBT, 15% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 BK001 HS PBT, unfilled, improved impact, heat stabilized, black Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR15 BK002 WX21 PBT, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR15 NL100 PBT, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR20 NL100 XA20 PBT, 20% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR50 BK002 CA01 PBT/PET, 50% glass fiber reinforced, heat & UV stabilized, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR50 NL100 PBT, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 NL TD22 PBT/PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecopet® PT70 GR15 NL100 PR PET, 15% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR30 NL100 PBT, 20% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecodur® PB70 GR35 NL100 HS01 PBT/PET, 35% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecopet® PT70 GR45 NL100 PR PET, 45% glass fiber reinforced, heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecopet® PT74 CR30 BK111 PR PET, 30% carbon fiber reinforced, black, fast crystallization grade Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | Throat |
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Feed Temperature | 50.0 - 70.0 °C | 122 - 158 °F | |
3M Dyneon™ 301Z Translucent Perfluoroelastomer System Features and Benefits:Excellent plasma resistance with low particle count Low extractables, low outgassing, and low particle generation for ultra high purity applicationsPhosphorous-free and silica.. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom for Electronic and Electric Standard Molding |
Mitsui Arlen™ AE4200 Modified Nylon 6T, for Tribolic Applications (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |
|||
Feed Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Hopper Bottom for Electronic and Electric Standard Molding |
Mitsui Arlen™ C215 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it possesses .. |