Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Drying Temperature = 194 °F Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301/GF/30/TF/15 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-0793 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7578 PPS, linear, with glass fiber and PTFE, improved wear resistance
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7648/BK PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7661/RD PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Improved fr..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7815 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Electrically ..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8066 PPS, linear, with carbon fiber, lubricant modified, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8077 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricity.S..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8095 PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.High chemic..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8148 PPS, linear, with PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage, isotropic shrinkage ..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8306 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Improved friction and wear behaviour. Emergency running property.Inherent flam..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8367 PPS, linear, with CNT
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. ..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8400 PPS, linear, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8456 PPS, linear, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8457 PPS, linear, with carbon fiber, lubricant modified
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.Strong, stiff parts.Suitable fo..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8524 PPS, linear, with glass fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 60.0 - 90.0 °C

@Time 7200 - 10800 sec
140 - 194 °F

@Time 2.00 - 3.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® TPU-7682 Thermoplastic polyurethane, with carbon fiber
Applications: Electrically conductive, suitable for continuous discharging of statically generated electricity.Improved wear behaviour, low warpage.Bearings, sleeves, sliding elements, chair rollers..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-7629/EG PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8060 PPS, linear, with glass fiber and PTFE, high viscosity
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.Low warpage, isotropic shrinkage characteristics.Improved friction and wear be..
Drying Temperature 60.0 - 90.0 °C

@Time 7200 - 10800 sec
140 - 194 °F

@Time 2.00 - 3.00 hour
Dehumidifying dryer
Lehmann & Voss LUVOCOM® 100-7126 VP Thermoplastic polyurethane, with PTFE
Applications: Improved friction and wear behaviour. Emergency running property.dynamic stressBearings, sleeves, sliding elements, chair rollers, handles.Information provided by Lehmann & Voss & Co.K..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301/CF/10/GF/20/GK/20/BK100 PPS, linear, with carbon fiber, glass fiber and micro glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-0824 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous disc..
Drying Temperature 50.0 - 90.0 °C

@Time >=14400 sec
122 - 194 °F

@Time >=4.00 hour
Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Copyright © lookpolymers.com All Rights Reserved