Processing Properties | Metric | English | Comments |
---|---|---|---|
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Pot Life | 90 min | 90 min | |
Resin Technology Group 401 Oxy-Bond™ Electrically Conductive Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | 90 min | 90 min | |
Resin Technology Group 401 Oxy-Bond™ Electrically Conductive Epoxy Adhesive Oxy-Bond and Millenium Adhesive SystemsEngineered for strength, durability, lightness, and formability, our Oxy-Bond and Millenium lines offer adhesives with physical and electrical properties to ma.. |
|||
Pot Life | >= 90 min | >= 90 min | |
Abatron 225 A/B Filled Potting Compound
(discontinued **) Dielectric structural potting and embedding adhesive. Higher impact, green and most colors. 10/3 variable ratio.Information provided by Abatron. |
|||
Pot Life | 90 min | 90 min | |
Huntsman HZ 340 Polyamide Approx. H+ equivalent weight 113. Mix Ratio with GY 6010 is 120.Comments/Applications: Solvent free, water-based polyamide with good adhesion. For use in coatings for plaster, concrete, masonry, .. |
|||
Pot Life | 90 - 150 min | 90 - 150 min | Time before parts must be mated |
Lord Adhesives 312 General Purpose, Low Viscosity Epoxy Adhesive Lord Epoxy AdhesivesLord® Epoxy Adhesives create superior bonds for rubber, SMC, plastics and metals. Our epoxy adhesives are widely used in the automotive industry, over 10 million cars and ligh.. |
|||
Pot Life | 90 - 120 min @Temperature 25.0 °C |
90 - 120 min @Temperature 77.0 °F |
54g mass |
Lord Adhesives Fusor® 309-1D / 309-2D Epoxy Adhesive Lord® 309 is a high performance, thixotropic, two-part epoxy adhesive that is used for applications that require gap filling or non-slumping characteristics on a vertical substrate. The cured adh.. |
|||
Pot Life | 90 - 105 min | 90 - 105 min | |
ITW Plexus Plexusâ„¢ MA590 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, long open time product and bond lines up to 1" thickInformation provided by Illinois .. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Curing |
Silikony Polskie Gumosil M Silicone Rubber Flexible with good tearing resistance |
|||
Pot Life | >= 90 min | >= 90 min | 100 gram mass |
Master Bond EP21ANHT Two Component, Room Temperature Curing Epoxy Adhesive Product Description: Master Bond Polymer Adhesive EP21ANHT is a two component room temperature curing adhesive, sealant and coating that combines high thermal conductivity and electrical insulation .. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21AOLV-1 Two Part, Room Temperature Curing Epoxy System Product Description: Master Bond Polymer Adhesive EP21AOLV-1 is a two component, thermally conductive, electrically isolating epoxy adhesive, sealant and coating. This versatile system will adhere t.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21NDFG Two component epoxy compound for high performance applications Product Description: Master Bond EP21NDFG is a two component, room temperature curing epoxy adhesive featuring outstanding physical properties, easy processing and a non-drip, paste-like consistency.. |
|||
Pot Life | >= 90 min | >= 90 min | 100 gram mass |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |
|||
Pot Life | >= 90 min | >= 90 min | 100 gram mass |
Master Bond EP21TDC-4ND Two component, highly flexibilized epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDC-4ND is a two component, very flexible epoxy system for high performance bonding, sealing and coating with a non-drip consistency. It has a one to four mix ra.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TDCHTND Versatile, toughened two component epoxy for bonding, sealing and coating Product Description: Master Bond EP21TDCHTND is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and exceptional user friendliness. It has a very forgiving.. |
|||
Pot Life | 90 - 150 min | 90 - 150 min | 100 grams |
Master Bond EP21FRNS-2 Two Component, Flame Resistant Epoxy System Master Bond Polymer System EP21FRNS-2 is a two component, room temperature curing, flame retardant compound for potting, encapsulating and casting. Particularly noteworthy are its low smoke generati.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | 100 gram mass |
Master Bond EP21TPFL-1AO Two Part, Flexible, Lower Viscosity Epoxy Polysulfide System Product Description: Master Bond EP21TPFL-1AO is a two component, low viscosity epoxy polysulfide for high performance bonding, sealing, coating and casting offering thermal conductivity, electrical.. |
|||
Pot Life | 90 min | 90 min | 25 grams |
Tra-Con Tra-Bond 2110 High Impact Epoxy Staking Compound TRA-BOND 2110 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Pot Life | 90 min | 90 min | 100 grams |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Pot Life | 90 min | 90 min | |
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy Material Description: A two component, optically clear, flexible epoxy adhesive designed for optical applications within semiconductor, fiber optic and medical industries. An alternative to EPO-TEK.. |
|||
Pot Life | 90 min | 90 min | |
Epoxy Technology EPO-TEK® 320-3 Optically Opaque Epoxy Material Description: A two component, black-colored and optically opaque epoxy designed for optical, medical, and opto-electronic packaging of semiconductor devices and components. It is a modific.. |
|||
Pot Life | 90 min | 90 min | |
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p.. |
|||
Pot Life | 90 min | 90 min | |
Epoxy Technology EPO-TEK® OE188 High Temperature Silica-Filled Epoxy Product Description: EPO-TEK® OE188 is a low CTE, designed for semiconductor and fiber optic applications. Advantages & Application Notes: Paste-like viscosity allows for application by dispensing.. |
|||
Pot Life | 90 min @Temperature 25.0 °C |
90 min @Temperature 77.0 °F |
500 g |
Abatron AboCast 8503-4/AboCure 8503-4 Colorless Epoxy AboCast 8503-4/AboCure 8503-4 is a general purpose, moderate speed, colorless epoxy casting compound with low viscosity. It offers a convenient 2/1 ratio by volume and lends itself to casting of thi.. |
|||
Pot Life | 90 min @Temperature 25.0 °C |
90 min @Temperature 77.0 °F |
500 g |
Abatron AboCast 8503-7/AboCure 8503-7 Colorless Epoxy AboCast 8503-7/AboCure 8503-7 is a general purpose, slow hardening, colorless epoxy casting compound with low viscosity. It is similar to the 8503-4 system, but more flexible. Suggested Uses: Trans.. |
|||
Pot Life | 90 min @Temperature 25.0 °C |
90 min @Temperature 77.0 °F |
|
BCC Products BC 9040 T Silicone RTV Rubber BC 9040T is a clear, addition/platinum cure, two-component, flowable compound that, regardless of thickness or confinement, cures at room temperature or by application heat. The cured rubber is high.. |
|||
Pot Life | 90 min | 90 min | 10 grams |
Tra-Con Tra-Duct 2929 Room Temperature Conductive Flexible Silver Epoxy Adhesive TRA-DUCT 2929 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy a.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1282 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |
|||
Pot Life | 90 - 120 min | 90 - 120 min | Mass: 100g; TM R050-19 |
Resinlab® EP1282 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP1282 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It is recognized under the Component Recognition Program of Underwriters Laborat.. |