Huntsman HZ 340 Polyamide

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman HZ 340 Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Approx. H+ equivalent weight 113. Mix Ratio with GY 6010 is 120.Comments/Applications: Solvent free, water-based polyamide with good adhesion. For use in coatings for plaster, concrete, masonry, asbestos, cement and nuclear facilities.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 18000 - 23000 cP
18000 - 23000 cP
Processing Properties Metric English Comments
Pot Life 90 min
90 min