Processing Properties | Metric | English | Comments |
---|---|---|---|
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 241-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and NSF 51 f.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Vyram™ 9101-65 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing characteristi.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Vyram™ 9203-45 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is designed for applications requiring good flexibility, appearance and sealing character.. |
|||
Vent Depth | 0.00254 - 0.00381 cm | 0.00100 - 0.00150 in | |
LG Chemical Lupox® PBT-GP-2150 15% GFR PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Vent Depth | 0.00254 - 0.00381 cm | 0.00100 - 0.00150 in | |
LG Chemical Lupox® PBT-GP-2156F 15% GFR Flame Retardant PBT General Purpose PBT, 15% Glass Fiber Reinforced, Weather Resistant, Flame Retardant, Non-Bleed. Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Vent Depth | 0.00254 - 0.00381 cm | 0.00100 - 0.00150 in | |
LG Chemical Lupox® PBT-HI1002F Impact Modified, Flame Retardant PBT Alloy Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Vent Depth | 0.00254 - 0.00381 cm | 0.00100 - 0.00150 in | |
LG Chemical Lupox® PBT-HI1002FM Impact Modified, Flame Retardant PBT Information provided by US distributor Polymer Technology and Services, LLC (PTS). |
|||
Vent Depth | 0.00254 - 0.00762 cm | 0.00100 - 0.00300 in | |
LTL Color Compounds ColorFast® PC100 Polycarbonate 10 melt standard injection molding gradeAll information provided by LTL Color Compounders, Inc. |
|||
Vent Depth | 0.00254 - 0.00762 cm | 0.00100 - 0.00300 in | |
LTL Color Compounds ColorFast® PC150 Polycarbonate 15 melt high flow polycarbonateAll information provided by LTL Color Compounders, Inc. |
|||
Vent Depth | 0.00254 - 0.00762 cm | 0.00100 - 0.00300 in | |
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 201-87 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 241-80W236 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with NSF 61 for plumbing applications in contact with potable water and contains.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 251-70W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 251-80W232 Thermoplastic Elastomer A soft, colorable, flame retardant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material has good fluid resistance and contains non-ether brominated flame retard.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 271-55 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 271-64 Thermoplastic Elastomer A soft, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as t.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 8211-65 Thermoplastic Elastomer A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 8281-65MED Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated use, as well as those.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 8281-90MED Thermoplastic Elastomer A hard, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 111-73 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 111-80 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Vent Depth | 0.00254 - 0.00762 cm | 0.00100 - 0.00300 in | |
LTL Color Compounds ColorFast® FRPS200 Styrene, High Impact V0/5VA high impact styreneAll information provided by LTL Color Compounders, Inc. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 221-80 Thermoplastic Elastomer
(discontinued **) A soft, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 221-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide.. |
|||
Vent Depth | 0.00254 cm | 0.00100 in | |
ExxonMobil Santoprene® 241-45 Thermoplastic Elastomer