Polymer Property : Injection Pressure = 85.0 MPa Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 230 PET - PBT 30% Glass Reinforced Polyester
Vypet VNT 230 is a 30% fiberglass reinforced modified PBT/PET polyester injection molding compound designed for electrical applications requiring improved surface aesthetics and improved UV resistan..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 245 PET - PBT 45% Glass Reinforced Polyester
Vypet VNT 245 is a 45% fiberglass reinforced modified PBT / PET polyester injection molding compound designed for electrical and automotive applications requiring low warp and improved surface finis..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 325 PET 25% Glass - Mineral Reinforced
Vypet 325 is a 25% glass/mineral reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Good balance resilience-stiffne..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 335 PET 35% Glass - Mineral Reinforced
Vypet VNT 335 is a 35% glass/mineral reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityT..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 615 FR PET 15% Glass Reinforced, Flame Retardant
Vypet VNT 615 FR is a 15% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant
Vypet VNT 630 FR is a 30% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 645 PET 45% Glass Reinforced
Vypet VNT 645 is a 45% glass reinforced PET injection molding compound designed for electrical and structural applications.Features: High temperature performance; Excellent strength and stiffness; E..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 835 PET 35% Glass-Mineral Reinforced
Vypet VNT 835 is a 35% mineral and fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional s..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 930 PET 30% Glass Reinforced
Vypet VNT 930 is a 30% fiberglass reinforced PET injection molding compound designed for structural applications.Features: High temperature performance; Low warp; Excellent dimensional stabilityTypi..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYTEEN PCGF10BK PC 10% Glass Reinforced
Vyteen PCGF10BK is a 10% fiberglass reinforced general purpose Polycarbonate grade.Features: - Good processabilityTypical Applications: - Laptop computer docking - Laser printer gear - Toner car..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET PBT 6300 BK PBT Unreinforced, Impact Modified
Vypet PBT 6300 BK is an unreinforced PBT injection molding compound offering excellent dimensional stability, chemical resistance, low moisture absorption and good electrical properties.Features: Hi..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 215 PET - PBT 15% Glass Reinforced Polyester
Vypet VNT 215 is a 15% fiberglass reinforced PET/PBT injection molding compound designed for structural applications.Features: High temperature performance; Low warp; High quality surfaceTypical App..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 615 PET 15% Glass Reinforced
Vypet VNT 615 is a 15% fiberglass reinforced PET injection molding compound designed for structural applications.Features: Easy, fast processing; Excellent strength and stiffness; Excellent dimensio..
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent..