Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 30% Glass Reinforced , Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
Manufacturer Lavergne Performance Compounds
Trade Name VYPET
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lavergne VYPET VNT 630 FR PET 30% Glass Reinforced, Flame Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vypet VNT 630 FR is a 30% fiberglass reinforced flame retardant PET injection molding compound designed for electrical and structural applications.Features: Flame retardant; UL yellow card file E216152; Excellent strength and stiffness; Excellent dimensional stabilityTypical Applications: Electrical parts; Appliances; Electronic applicationsInformation provided by Bieglo Gmbh for Lavergne Performance Compounds
Physical Properties Metric English Comments
Density 1.65 g/cc
0.0596 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 2.00 mm
0.0020 in/in

@Thickness 0.0787 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0090 cm/cm

@Thickness 2.00 mm
0.0090 in/in

@Thickness 0.0787 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 145 MPa
21000 psi
5 mm/min; ASTM D638
Flexural Strength 215 MPa
31200 psi
1.3 mm/min; ASTM D790
Flexural Modulus 10.2 GPa
1480 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.900 J/cm

@Temperature 23.0 °C
1.69 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 228 °C
442 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 0.850 mm
V-0

@Thickness 0.0335 in
5VA

@Thickness 1.50 mm
5VA

@Thickness 0.0591 in
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
Glow Wire Test 825 °C
1520 °F
GWIT at 1.0 mm; IEC 60695-2-13
960 °C
1760 °F
GWFI at 1.0 mm; IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 29.0 kV/mm
737 kV/in
ASTM D149
Comparative Tracking Index 15 - 30 V
15 - 30 V
UL746
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Middle Barrel Temperature 265 - 275 °C
509 - 527 °F
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Nozzle Temperature 275 - 295 °C
527 - 563 °F
Melt Temperature 275 - 295 °C
527 - 563 °F
Mold Temperature 95.0 - 120 °C
203 - 248 °F
Injection Pressure 55.0 - 85.0 MPa
7980 - 12300 psi