Processing Properties | Metric | English | Comments |
---|---|---|---|
Injection Pressure | 2.76 - 8.27 MPa | 400 - 1200 psi | |
RheTech Products FRP255-01 Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Injection Pressure | 7.24 - 8.27 MPa | 1050 - 1200 psi | |
Ravago Manufacturing Americas Hylac® GP74G30 ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant ABS4500G30 ABS, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol BR2029 Nylon 66, General Purpose, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol BR4014BK ABS, High Gloss, Black Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA112 Nylon 66, Nucleated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA123 Nylon 66, Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA133G33 Nylon 66, 33% Glass Fiber, Highly Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA211G40 Nylon 6, 40% Glass Fiber, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA211N40 Nylon 6, Mineral/Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213 Nylon 6, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA213G33 Nylon 6, 33% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA223G13 Nylon 6, 13% Glass Fiber, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0004 Nylon 6 Alloy Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0010HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PA2SP0017 Nylon 6, Impact Modified Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PBTSP0006 Polyester Elastomer Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0005 Polycarbonate/ASA Alloy, Flame Retardant Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PCSP0017 Polycarbonate/Polyester Alloy, 30% Glass Reinforced Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PP1100N40CC Polypropylene Homopolymer, 40% Glass Fiber and Mineral Reinforced, Chemically Coupled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPSP0004 Polypropylene, Random Copolymer Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6601L Nylon 66, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6601M Nylon 66, Molybdenum Disulfide Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6608 HSL Nylon 66, High Impact Modified, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 6622-L Nylon 66, Glass Fiber Filled, Lubricated Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol 66B40 Nylon 66, 40% Glass Bead Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 4.96 - 8.27 MPa | 720 - 1200 psi | Secondary |
Clariant Renol PPSSP0001 Polyphenylene Sulfide, Glass Fiber and Bead Filled Data provided by Clariant Masterbatches |
|||
Injection Pressure | 7.24 - 8.27 MPa | 1050 - 1200 psi | |
Ravago Manufacturing Americas Hylac® GP30G ABS, 30% Glass Fiber Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |