Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 - 420 °C | 734 - 788 °F | Injection molding, extrusion |
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7678 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7835 PEEK, with glass fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts,.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8052/EM/BL PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8158 PEEK, with mineral filler Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8292 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8319 PEEK, with PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8320 PEEK, with aramid reinforcement and PTFE, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts.Improved friction and wear behaviour. Emergency r.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8350 PEEK, with carbon fiber, PTFE, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8416 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8476 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.High dimensionally stable precisio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 2205-7123 Blend based on polyaryl ether ketone, with carbon fiber, PTFE, lubricant modified Applications: High dimensionally stable precision parts, high continuous use temperature.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistanceChemical and hydr.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 2607-7921 Blend based on polyaryl ether ketone, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1104/XCF/30 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1104-7824 Polyether ketone, with carbon fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/BK7308 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High chemical resistance parts, non flammable.Suitable for biocompatible application.Not f.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/30/NAT-2 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/GY7993 PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0950/RD PEEK, unreinforced Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7310 PEEK, with glass fiber, easy flowing, low-warpage Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High dimensionally stable precision parts, high continuous use temperature.Superheated ste.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7536 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7594/BL PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7731/BL PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-7876-1 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Low warpage.Emergency running property.Information provided by Lehmann.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105/TF/20/NAT PEEK, with PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |
|||
Processing Temperature | 390 °C | 734 °F | mass temp |
Lehmann & Voss LUVOCOM® 1105-0918/BL PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |