Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 270 - 280 °C | 518 - 536 °F | Average value: 275 °C Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | Average value: 289 °C Grade Count:31 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Processing Temperature | 270 °C | 518 °F | mass temp |
Lehmann & Voss LUVOCOM® 3/CF/30 Polyamide 6, with carbon fiber Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressElectrically conductive, suitable.. |
|||
Processing Temperature | 270 °C | 518 °F | mass temp |
Lehmann & Voss LUVOCOM® 3-7088/GY7012 Polyamide 6, with carbon fiber and glass fiber, low-warpage Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Processing Temperature | 270 °C | 518 °F | mass temp |
Lehmann & Voss LUVOCOM® 3-7088-2 Polyamide 6, with carbon fiber and glass fiber, low-warpage, heat stabilized Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Strong, stiff parts.dynamic stressElectrically conductive, suitable for continuous discharging of staticall.. |
|||
Processing Temperature | 270 °C | 518 °F | mass temp |
Lehmann & Voss LUVOCOM® 3-7723/ EG Polyamide 6, with carbon fiber, high viscosity Applications: Automotive industry, textile machinery, apparatus- and precision engineering.High-strength and stiff parts; low coefficient of expansion.dynamic stressAntistatic.Handles, levers, rolle.. |
|||
Processing Temperature | 270 °C | 518 °F | mass temp |
Lehmann & Voss LUVOCOM® 3-8277 Polyamide 6, unreinforced Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce.. |
|||
Processing Temperature | 270 °C | 518 °F | mass temp |
Lehmann & Voss LUVOCOM® 55-7880 PC/ABS Alloy, with carbon fiber and glass fiber Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Strong, stiff parts.Reduced moment of inertia compared with me.. |
|||
Processing Temperature | <= 270 °C | <= 518 °F | |
Kingfa PET-G30 30% Glass Fiber Reinforced PET Features:High strengthGood heat resistanceApplications:Injection moldingApplication partsAuto partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Processing Temperature | 270 °C | 518 °F | |
Shinil Chemical SHINCON MPPO Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
Ter Hell Plastic Terez® PC 9007 UV Polycarbonate Description: Crystal clear, low viscosity Polycarbonate with mold release and UV-stabilized.Application: For thin-walled injection molded parts.Information provided by Ter Hell Plastic GMBH. |
|||
Processing Temperature | 270 °C | 518 °F | Extruder Temperature |
DSM Akulon® F130-C2 PA6 Medium Viscosity, Film Extrusion, Lubricated |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecomid® NA30 GR50 BK002 XA40 PA6.6, 50% glass fiber reinforced, flame retardant, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
Eurotec® Tecomid® NA40 GR25 NL HS PA6.6, 25% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
Eurotec® Tecomid® NA40 GR30 NL RT PA6.6, 30% glass fiber reinforced, PTFE modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
Eurotec® Tecomid® NAX0 GR60 NL PA6.6, 60% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 HT PET, 30% glass fiber reinforced, high heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TA210HS , Heat Stabilized PA66, DAM Heat stabilizedInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TA250GFR , Flame Retardant, 25% Glass Fiber Reinforced PA66, DAM GF reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | |
E-Polymers TEKAMID® TB110M40 , 40% Mineral Filled PA6, DAM 40% Mineral filled, Heat resistance, PlatableInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
E-Polymers TEKAMID® TB120GM20 , 20% GF/MF Reinforced PA6, DAM 20% GF/MF reinforced, Good surface, Low warpageInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
E-Polymers TEKANATE™ G710 , 10% Glass Fiber Reinforced Poly Carbonate 10% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
E-Polymers TEKANATE™ G715FR , Flame Retardant, 15% Glass Fiber Reinforced Poly Carbonate 15% Glass Fiber reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 330 °C | 518 - 626 °F | |
E-Polymers TEKANATE™ G730 , 30% Glass Fiber Reinforced Poly Carbonate 30% Glass Fiber reinforcedInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
Eurotec® Tecomid® NA40 CR20 BK111 PA6.6, 20% carbon fiber reinforced, black Information provided by Eurotec® |
|||
Processing Temperature | 270 - 310 °C | 518 - 590 °F | |
Eurotec® Tecotek® PC43 GR20 BK002 PC, 20% glass fiber reinforced, black Information provided by Eurotec® |
|||
Processing Temperature | 270 - 300 °C | 518 - 572 °F | |
E-Polymers Tekaster® F615G45 , 45% Glass Fiber Reinforced PET 45% Glass Fiber reinforced, High strength, Information provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | 270 - 290 °C | 518 - 554 °F | Extrusion |
Arkema Group Rilsan® Clear G170 Polyamide Rilsan® Clear G170 is a high performance transparent polyamide with outstanding thermal resistance. This grade has been designed for extrusion and injection molding applications and for medical use.. |
|||
Processing Temperature | 270 °C | 518 °F | Injection, recommended |
Arkema Group Rilsan® Clear G380 Renew Polyamide Rilsan® Clear G830 Rnew is a high performance transparent polyamide partially based on renewable resources. This grade has been specially designed for injection molding applications, ideally suited.. |