Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | <= 260 °C | <= 500 °F | |
Ineos Nova 1552 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Easy processing, High modulus, Improve stress whitening, Custom colorsApplications: Injection molding, Office furniture, Electronic media, Photographic equipmentPerformance grades of polystyrene are.. |
|||
Processing Temperature | 260 °C | 500 °F | See Materials Notes |
BASF Capron® 8200 HS BK-102 Nylon 6 (Dry)
(discontinued **) Capron 8200 HS BK-102 is a medium viscosity, heat stabilized, pigmented black, nylon 6 injection molding homopolymer exhibiting resistance to sink-mark formation in thick section, and improved tough.. |
|||
Processing Temperature | <= 260 °C | <= 500 °F | |
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelPower toolComputer and acce.. |
|||
Processing Temperature | 260 °C | 500 °F | Stress Relieving |
Mueller Alloy 3600 Free Cutting Brass (UNS C36000) Machinability: Recently amended and revised to reflect a lower maximum lead percentage; C36000 remains the industry standard for general machining and high volume production. The excellent machinabi.. |
|||
Processing Temperature | 260 °C | 500 °F | |
Shinil Chemical SHINCON PC Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Processing Temperature | 260 °C | 500 °F | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Engine Cover SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Processing Temperature | 260 °C | 500 °F | |
Shinil Chemical SHINNANO PA-66 Polymer Nanocomposite Window Strip SHINNANO is the product line of polymer nanocomposite made by dispersing nano fillers, mainly, NANOCLAY. Recently, Shinil has developed varios nanocomposite grades for automotive applications using.. |
|||
Processing Temperature | 260 °C | 500 °F | |
Tipco Tipcofil® AG 600 - 30% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 30% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Processing Temperature | 260 - 282 °C | 500 - 540 °F | |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Processing Temperature | 260 - 282 °C | 500 - 540 °F | |
Eastman Tritan TX2001 Copolyester Eastman Tritan TX2001 is an amorphous copolyester with excellent appearance and clarity. Eastman Tritan TX2001 contains a mold release derived from vegetable based sources. Its most outstanding fe.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | ISBM Processing Melt Temp. |
Eastman Tritan WX510 Copolyester Eastman Tritan WX510 is a transparent blue resin specifically developed for blow molded bottles. Extremely high melt strength makes the resin an excellent choice when manufacturing large bottles. .. |
|||
Processing Temperature | <= 260 °C | <= 500 °F | |
DuPont™ Bynel® 41E710 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 NL FA50 PA6.6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 NL IM PA6.6, impact modified, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecomid® NA40 NL XA70 PA6.6, unfilled, flame retardant - halogen free (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 GR15 NL100 PS20 PET, 15% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
E-Polymers TEKAMID® TB120G15T Impact Modified, 15% Glass Fiber Reinforced PA6, DAM 15% GF reinforced, Good impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | <= 260 °C | <= 500 °F | |
DuPont™ Bynel® 41E766 Anhydride Modified LLDPE BYNEL® Series 4100 series resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All BYNEL Series 4100 series resins are available in pellet form for use in conventional ext.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecodur® PB70 GR45 NL100 HS01 PBT/PET, 45% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 GR30 NL100 PS20 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural, fast crystallization grade Information provided by Eurotec® |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Processing Temperature | 260 °C | 500 °F | Recommended Extrusion Temperature |
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | |
E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy High impact, weather resistance, chemical resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Processing Temperature | <= 260 °C | <= 500 °F | |
Ineos Nova 8049 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High gloss at 60°=95; at 20°C=90, Improved scuff resistance, Custom colorsApplications: Injection molding, Cost effective replacement for some ABS applications, Excellent for applications where hi.. |
|||
Processing Temperature | <= 260 °C | <= 500 °F | |
Ineos Nova 817 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow crystal polystyrene, Custom colorsApplications: Injection molding, Designed for use in high speed, Thin section applications and complex parts designs where custom coloring is a requiremen.. |
|||
Processing Temperature | 260 - 280 °C | 500 - 536 °F | Resin Temperature |
Asahi Kasei Xyron® A0100 PPE/PA AutomotiveInformation provided by Asahi Kasei |
|||
Processing Temperature | <= 260 °C | <= 500 °F | |
Styrolution NAS® 21 Acrylic Copolymer Features:Sparkling clarity Scratch resistant Can be blended with K-Resin at any level to modify flexibility, surface hardness, heat distortion temperatures, etc. Styrenic processing advantages Gamma.. |
|||
Processing Temperature | 260 °C | 500 °F | |
Tipco Tipcofil® AGM 802 - 25% Mineral & 15% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 25% Mineral + 15% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |