Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2EU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® HP2REU PC (Europe-Africa-Middle East) Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a h.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 95.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Lexan® AD4820 PC (Asia Pacific) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE1GFN1 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN1 is a 10% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific) Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics XYLEX HX7509HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, polycarbonate/Polyester alloy; contains mold release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), fo.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP THERMOCOMP BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313I PC (Asia Pacific) DX06313I is 30% glass fiber reinforced, impact modified polycarbonate resin. High flow and good ductility. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HH180 PPE+PS Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Asia Pacific) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL HH180 PPE+PS (Europe-Africa-Middle East) Noryl* HH180 is a high heat, unfilled modified polyphenylene ether resin with a Vicat B/120 temperature of 185 deg C. Noryl HH180 is only available in color 80365. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Asia Pacific) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH7114 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH7114 resin is a 20% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve UL94 flame ratings while offering an exceptional balance of streng.. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
37.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP WC006 PBT LNP* THERMOCOMP* WC006 is a compound based on PBT resin containing 30% Carbon Fiber. Added feature of this grade is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
37.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOTUF MF004AI PP (Asia Pacific) LNP* Thermotuf* MF004AI is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
CTE, linear, Transverse to Flow | 68.0 µm/m-°C @Temperature -30.0 - 80.0 °C |
37.8 µin/in-°F @Temperature -22.0 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |