Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 0.000 - 100 °C |
30.6 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E831 |
Solvay Specialty Polymers Amodel® AE-8133 Polyphthalamide (PPA)
(discontinued **) Amodel AE-8133 is a 33% glass reinforced polyphthalamide (PPA) designed to work in the modern automotive electrical environment. This grade features a high heat deflection temperature, high flexural.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 °C |
30.6 µin/in-°F @Temperature 73.4 °F |
ASTM D696 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 200 °C |
30.6 µin/in-°F @Temperature 392 °F |
ASTM D696 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL SE1GFN3 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN3 is a 30% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
30.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific) LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1010KM PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1100FV PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1110FV PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem 1110FV PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data was supplied by SABIC-I.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1110V PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 9011 PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem DT1800E PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM DT1810EV PEI Blend Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM EXUM0169 PEI Blend (Asia Pacific) Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON DEF42 PC LNP STAT-KON* DEF42 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
30.6 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® XK2340 Polyphenylene Sulfide Alloy (PPS Alloy), 40% Glass Fiber Ryton® XK2340 40% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength, toughness, and rigidity, along with excellent flow in thin-walled parts, low .. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
30.6 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 150 °C |
30.6 µin/in-°F @Temperature 73.4 - 302 °F |
ISO 11359-2 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics Ultem 1010KM PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
30.6 µin/in-°F @Temperature -58.0 - 122 °F |
TMA; ASTM E831 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature <=250 °C |
30.6 µin/in-°F @Temperature <=482 °F |
z (< Tg); IPC TM-650 2.4.24 |
Arlon 85N Polyimide Laminate and Prepreg 85N is a polyimide and laminate prepreg system for PWBs requiring resistance to high temperature, both in process and in end-use application. Bromine-free chemistry provides thermal stability for a.. |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
30.6 µin/in-°F @Temperature 73.4 - 131 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 55.0 µm/m-°C @Temperature -40.0 - 150 °C |
30.6 µin/in-°F @Temperature -40.0 - 302 °F |
ASTM E 831 |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |