Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Transverse to Flow = 30.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 0.000 - 100 °C
30.6 µin/in-°F
<br>@Temperature 32.0 - 212 °F
ASTM E831
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA) &nbsp;(Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East)
Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 1010P PEI
Enhanced flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 1100EF PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Ultem 1100FV PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 1100V PEI
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East)
Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM CRS5011R PEI (Asia Pacific)
Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem DT1800E PEI Blend
Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem DT1810E PEI Blend
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Americas re..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem DT1810E PEI Blend (Asia Pacific)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacifi..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem DT1810EV PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming, UL94 V0 listed.This data was supplied by SABIC-IP for..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem EXUM0169 PEI Blend (Europe-Africa-Middle East)
Improved ductility, transparent, enhanced flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Afri..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -20.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU1004 PEI
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -20.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU1100 PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East)
Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics ULTEM HU1110 PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM SF2350 PEI Blend
High flow Ultem blends for thin wall application
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM UF5011S PEI
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem 1010KM PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature 23.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM UF5011S PEI (Europe-Africa-Middle East)
Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming.
CTE, linear, Transverse to Flow 55.0 µm/m-°C
<br>@Temperature -40.0 - 150 °C
30.6 µin/in-°F
<br>@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant.
Copyright © lookpolymers.com All Rights Reserved