Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 365 PC+PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 365 PET (Asia Pacific) Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031"". |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66 (Asia Pacific) LNP* Stat-kon* REL42 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermocomp IFB33 PA 6/12 (Asia Pacific) LNP* Thermocomp* IFB33 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Americas regi.. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific) LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Lubricomp KCL22 Acetal Copoly LNP* Lubricomp* KCL22 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 95.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 203 °F |
ASTM E 831 |
SABIC Innovative Plastics Valox® 365 PET Unreinforced, opaque, provides chemical resistance and dimensional stability, UL94V-0 rated at 0.031".This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 79.2 µm/m-°C @Temperature -40.0 - 40.0 °C |
44.0 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP STAT-KON RD000 PA 66 LNP STAT-KON* RD000 is a compound based on Nylon 66 resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |