Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 80.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 176 °F
ISO 11359-2
SABIC Innovative Plastics LNP KONDUIT OX11314 PPS (Europe-Africa-Middle East)
Thermally conductive mineral and glass fiber filled PPS Eco-FR compound
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature <=162 °C
11.7 µin/in-°F

@Temperature <=324 °F
Below Tg; ISO 11359
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 150 - 200 °C
11.7 µin/in-°F

@Temperature 302 - 392 °F
4
Solvay Specialty Polymers Amodel® A-8422 LS WH159 Polyphthalamide (PPA), 22% Mineral
Amodel® A-8422 LS is a light-stabilized, high-reflectivity, 22%-reinforced white polyphthalamide (PPA) that exhibits high heat resistance, high strength and stiffness over a broad temperature ran..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 150 - 200 °C
11.7 µin/in-°F

@Temperature 302 - 392 °F
4
Solvay Specialty Polymers Lavanta® 5115 WH 011 Polyester, High Performance (HPP), 15% Glass Fiber
Lavanta® 5115 WH011 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount ..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 150 °C
11.7 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Valox® ENH8560 PBT+PET (Europe-Africa-Middle East)
Non-Brominated & Non-Chlorinated Flame Retardant, 30% Glass fiber reinforced PBT/PET blend
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ507 PBT+PC
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific)
PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump ..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 150 °C
11.7 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 150 °C
11.7 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Europe-Africa-Middle East)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Afr..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 150 °C
11.7 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 150 °C
11.7 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX103R PEI+PCE
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Americas r..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 150 °C
11.7 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 150 °C
11.7 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
SABIC Innovative Plastics Ultem ATX103R PEI+PCE (Asia Pacific)
30% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing in recognized colors.This data was supplied by SABIC-IP for the Asia Pacif..
Copyright © lookpolymers.com All Rights Reserved