Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.300 W/m-K @Temperature 260 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Pyrotek Pyrocast AR70 Low-Density Refractory Castable Pyrocast AR70 refractory castable is a high-strength, low-density refractory well suited for specific aluminum foundry applications.ApplicationsSprue Bushings for low pressure die casting Intermedia.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 400 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Pyrotek Pyrotherm M-68 Structural Insulation Board Pyrotherm M-68 is a calcium-silicate board designed for non-ferrous applications. M-68 offers a unique combination of low shrinkage, low thermal conductivity and non-wetting properties which make i.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 23.0 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 23.0 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 100 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 212 °F |
ASTM E1530 |
3M Dyneon™ 1750 PTFE Powder
(discontinued **) Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 250 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CC503 PTFE, 15% Mineral Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings - FDA compliant, valve seats, seals.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 250 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 250 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E1530 |
3M Dyneon™ CC605 PTFE 25% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.300 - 0.380 W/m-K @Temperature 1000 °C |
2.08 - 2.64 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 1.2.4. MIX GM Refractory Insulating Castable Description: This light weight gunning castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Re.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 1425 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 2597 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 1425 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 2597 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 1425 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 2597 °F |
parallel to thickness; ASTM C177 |
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 1425 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 2597 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 538 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 1000 °F |
ASTM C182 |
BNZ Materials BNZ-25 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 816 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-26-60 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 1000 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials BNZP-23 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 600 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 600 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials Color B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.300 W/m-K @Temperature 260 °C |
2.08 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials PA 26 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.300 - 0.400 W/m-K @Temperature 200 °C |
2.08 - 2.78 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast FI 25-12 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |