Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon.
Physical Properties Metric English Comments
Bulk Density 0.720 g/cc
0.0260 lb/in³
ASTM D4894
Density 2.20 g/cc
0.0795 lb/in³
ASTM D4894
Particle Size 750 µm
750 µm
ASTM D4894
Deformation 4.0 %

@Pressure 15.00 MPa
4.0 %

@Pressure 2175 psi
ASTM D621
7.0 %

@Time 86400 sec,
Pressure 15.00 MPa
7.0 %

@Time 24.0 hour,
Pressure 2175 psi
ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 57
57
value after 15 sec; ASTM D2240
62
62
initial value; ASTM D2240
Tensile Strength at Break 20.7 MPa
3000 psi
ASTM D4894
Elongation at Break 280 %
280 %
ASTM D4894
Tensile Modulus 0.0931 GPa
13.5 ksi
ASTM D638
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C

@Temperature 30.0 - 100 °C
31.7 µin/in-°F

@Temperature 86.0 - 212 °F
139 µm/m-°C

@Temperature 100 - 200 °C
77.0 µin/in-°F

@Temperature 212 - 392 °F
ASTM E831
171 µm/m-°C

@Temperature 200 - 300 °C
95.0 µin/in-°F

@Temperature 392 - 572 °F
ASTM E831
Thermal Conductivity 0.300 W/m-K

@Temperature 250 °C
2.08 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM E1530
0.320 W/m-K

@Temperature 100 °C
2.22 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
Shrinkage 1.9 %
1.9 %
ASTM D4894